聚苯胺长效防腐水性环保涂料的研制及性能研究
2013-06-03 14:07:38
作者:康先进等来源:=$docheckrep[1]?ReplaceBefrom($ecms_gr[befrom]):$ecms_gr[befrom]?>
摘要:采用原位化学合成法制备对甲苯磺酸掺杂的聚苯胺/二氧化硅复合材料,并用红外光谱、扫描电镜和透射电镜表征其结构,以合成的聚苯胺/二氧化硅为功能组分,丙烯酸水性乳液为成膜物质,制成水性环保防腐涂料。用电化学测试技术研究复合水性防腐涂料对碳钢基材的防护效果。结果表明,复合水性防腐涂料使金属基体的腐蚀电位正移,具有较好的钝化效果,增强了耐蚀性。
Absract:Polyaniline-SiO2 was in situ synthesized and doped by p-toluenesulfonic acid (p-TSA). The composites were characterized by FTIR, SEM and TEM. The corrosion performance of polyaniline-SiO2 pigmented waterborne coating on carbon steel was studied by electrochemical testing technique in 3.5% NaCl solution. The tested results showed that a passivation effect and a positive shift of corrosion potential occurred due to the application of coating on metals and the anticorrosion property was enhanced.
Key Word:polyaniline ,SiO2,waterborne coating,polarization
Absract:Polyaniline-SiO2 was in situ synthesized and doped by p-toluenesulfonic acid (p-TSA). The composites were characterized by FTIR, SEM and TEM. The corrosion performance of polyaniline-SiO2 pigmented waterborne coating on carbon steel was studied by electrochemical testing technique in 3.5% NaCl solution. The tested results showed that a passivation effect and a positive shift of corrosion potential occurred due to the application of coating on metals and the anticorrosion property was enhanced.
Key Word:polyaniline ,SiO2,waterborne coating,polarization
相关文章
无相关信息
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62313558-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
铝合金LDH自修复自抗菌膜层构建
点击数:2727
碳钢及合金钢应用与区别
点击数:2609