自锚式悬索桥混凝土主塔防腐涂装研究与应用
2013-06-03 14:31:28
作者:李庭波 黄卓著来源:=$docheckrep[1]?ReplaceBefrom($ecms_gr[befrom]):$ecms_gr[befrom]?>
摘要:研究了酸雨对混凝土的腐蚀机理,以实际工程为背景,对悬索桥混凝土主塔防腐涂装技术从设计、施工、检测等方面进行了论述,实践证明:采用封闭漆+ 中间漆+面漆的涂装体系,有效抵御了酸雨的腐蚀,有重要的推广价值。
Abstract:The paper researches the corrosive mechanism of the acid rain on the concrete,indicates the anti-corrosive coating technique of concrete main tower of the suspension bridge from the design,the construction and the inspection,and proves by the practice that the adoption of coating system with the sealing paint plus intermediate coat can prevent the corrosion of the acid rain,so it has important expansion value.
Key Word:acid rain,concrete main tower,anti-corrosive coating
Abstract:The paper researches the corrosive mechanism of the acid rain on the concrete,indicates the anti-corrosive coating technique of concrete main tower of the suspension bridge from the design,the construction and the inspection,and proves by the practice that the adoption of coating system with the sealing paint plus intermediate coat can prevent the corrosion of the acid rain,so it has important expansion value.
Key Word:acid rain,concrete main tower,anti-corrosive coating
相关文章
无相关信息
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62313558-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
铝合金LDH自修复自抗菌膜层构建
点击数:2727
碳钢及合金钢应用与区别
点击数:2609