研究背景 Introduction |
研究方法 Methods 该研究基于现有文献全面剖析了各类典型的蠕变寿命预测方法,将其主要划分为基于单轴应力状态的方法与基于多轴应力状态(蠕变裂纹扩展试样)的方法两大类 This study analyzes typical existing prediction methods based on available research, categorizing them primarily into uniaxial stress state-based methods and multiaxial stress state-based methods (utilizing creep crack growth specimens) |
研究亮点 Highlights
|
|
研究意义 Significance 该研究为工程实践中评估与选择合适的蠕变预测模型提供了关键指导。 This study provides vital guidance for evaluating and selecting appropriate creep prediction models in engineering practice. |
|
作者 Authors 该研究的作者为华东理工大学及上海飞行器力学与控制研究院的张坤博士、谈建平教授和涂善东院士。 This paper is authored by Dr. Kun Zhang, Prof. Jian-Ping Tan, and Prof. Shan-Tung Tu from the East China University of Science and Technology and the Shanghai Institute of Aircraft Mechanics and Control.
华东理工大学 涂善东 院士 Prof. Shan-Tung Tu, ECUST, China 涂善东院士:华东理工大学讲席教授、中国工程院院士。曾任南京工业大学和华东理工大学副校长。涂善东院士一直致力于高温结构完整性和工程领域的研究,包括蠕变、疲劳、断裂、结构完整性监测和高温装备设计。他已发表400余篇出版物,并获得国家科技进步奖、国家技术发明奖等多项殊荣。Prof. Shan-Tung Tu, Chair Professor at East China University of Science and Technology (ECUST) and Academician of the China Academy of Engineering. He previously served as the Vice President of Nanjing Tech University and ECUST. Prof. Tu has been long dedicated to research in the field of high-temperature structural integrity and engineering, including creep, fatigue, fracture, structural integrity monitoring, and high-temperature equipment design. He has authored over 400 publications and has been honored with numerous prestigious awards, such as the National Science and Technology Progress Award and the National Technological Invention Award. Dr. Kun Zhang obtained his Ph.D. from East China University of Science and Technology (ECUST) in 2023 under the supervision of Prof. Shan-Tung Tu and Prof. Jian-Ping Tan. In 2025, he joined the College of Mechanical Engineering at Zhejiang University of Technology. His research primarily focuses on the structural integrity of high-temperature materials, with specific interests in creep constraint effects, long-term creep life prediction, and small-specimen property measurement techniques. Kun Zhang, Jian-Ping Tan, Shan-Tung Tu, Effectiveness of the methods in predicting long-term creep rupture life of materials: a critical analysis, Materials at High Temperatures 42(5-6) (2025) 370–380. https://doi.org/10.1080/09603409.2025.2586361 |
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
官方微信
《腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62316606
- 邮箱:fsfhzy666@163.com
- 腐蚀与防护网官方QQ群:140808415