高周疲劳下含短裂纹晶体细观应力分析
2014-08-07 11:39:40
作者:本站整理来源:=$docheckrep[1]?ReplaceBefrom($ecms_gr[befrom]):$ecms_gr[befrom]?>
朱福先,周金宇,孙奎洲,韩文钦
江苏理工学院江苏常州 213001
摘要:采用随机平面voronoi图模拟晶体微观结构,基于有限元方法计算了高周疲劳下含短裂纹晶体细观应力。研究了短裂纹尖端晶体在不同晶向下的应力状态,分析了短裂纹的应力强度因子随晶向的变化规律。对短裂纹穿越晶界的扩展进行了数值模拟,研究分析了短裂纹扩展方向同晶向的变化规律。
关键字:高周疲劳;短裂纹;细观应力;强度因子;晶向
Microscopic Stress Analysis of Crystal with Short Crack under High Cycle Fatigue
ZHU Fuxian, ZHOU Jinyu, SUN Kuizhou, HAN Wenqin
Jiangsu University of Technology, Changzhou 213001 China
Abstract:The microscopic structure of crystal is simulated by the random plane voronoi diagram, and then based on finite element method the microscopic stress of crystal with short crack underhigh cycle fatigue are analyzed. After the study of the crystal stress before the crack tip,variation of stress intensity factors are discussed depending on the grain orientations. The numerical simulation of short crack propagation the through grain boundary is carried out to discuss the variation of the short crack propagating orientation with the grain orientations.
Key words: High cycle fatigue;Short crack;Microscopic stress;Grain orientation
联系方式
朱福先:glzhfx@sina.com
责任编辑:赵泽南
《中国腐蚀与防护网电子月刊》征订启事
投稿联系:刘娟 电话:010-82387968-807
QQ: 2850329508 邮箱:liujuan@ecorr.org
中国腐蚀与防护网官方 QQ群:140808414
相关文章
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62313558-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
铝合金LDH自修复自抗菌膜层构建
点击数:2727
碳钢及合金钢应用与区别
点击数:2609