US 6788075 B2 Anode monitoring
An anode monitoring system for monitoring the integrity of anodes 2 provided on a metallic structure such as a pipeline system 1. A signal circuit Sn including the pipeline 1 and one of the anodes 2 is set up and appropriate signals are looked for at a central station 4. Reception of the signal at the central station 4 is dependent on the integrity of the anode 2 under inspection at that time. If the anode 2 is missing or defective the expected signal is not received and thus the fault in the anode 2 can be detected. A notch filter 5 is inserted in series between each anode 2 and the pipeline 1. The filter 5 provides a high impedance which can be signalled across but does not interfere with the cathodic protection system.
阳极监测系统用于监测设置在金属结构如管道系统1的阳极2的完整性。设置一个包括管道1和一个阳极2的信号电路Sn并且在中心站4寻找适当的信号。接收信号的中心站4依赖于观察阳极2当时的完整性。如果阳极2缺失或没有接收到预期的信号,即可检测出故障在阳极2.陷波滤波器5被串联插入各阳极2和管线1间。滤波器5提供了一个高阻抗,可以表示整个阴极保护系统但不干扰。
责任编辑:郭静
《中国腐蚀与防护网电子期刊》征订启事
中国腐蚀与防护网官方 QQ群:140808414
相关文章
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62313558-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
铝合金LDH自修复自抗菌膜层构建
点击数:2727
碳钢及合金钢应用与区别
点击数:2609