Quantitative transient analysis of localized corrosion
US 7713405 B2
ABSTRACT
An electrochemical noise method, apparatus and system may be used to estimate and/or calculate parameters of interest related to corrosion rates of an electrically conductive article. The apparatus involves a working electrode (having substantially the same composition of the electrically conductive article), a reference electrode, and a counter electrode in an environment of interest. The working electrode is placed under potentiostatic control. A current transient between the working electrode and the counter electrode is measured. The working electrode is switched to open potential. A potential transient is measured over the duration of a localized corrosion event. The localized corrosion may then be calculated based on the measured potential transient and the current transient.
摘要
电化学噪声的方法,装置和系统可被用于估计和/或计算有关的导电性物品的腐蚀速率的感兴趣的参数。该装置包括一个工作电极(具有基本导电性物品的相同组合物),参比电极,并在感兴趣的环境中的对电极。将工作电极置于恒电位下的控制。在工作电极和对电极之间的电流瞬变的测量。在工作电极被切换到开路电势。在一个局部腐蚀事件的持续时间里一个瞬时电势被测量。局部腐蚀然后可以基于所测量的电势瞬间,电流瞬态计算。
责任编辑:郭静
《中国腐蚀与防护网电子期刊》征订启事
中国腐蚀与防护网官方 QQ群:140808414
相关文章
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62313558-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
铝合金LDH自修复自抗菌膜层构建
点击数:2727
碳钢及合金钢应用与区别
点击数:2609