中国城市供水管网腐蚀现状及其对水质的影响
2014-08-15 11:16:18
作者:本站整理来源:=$docheckrep[1]?ReplaceBefrom($ecms_gr[befrom]):$ecms_gr[befrom]?>
骆鸿1,刘智勇2,卢琳2,董超芳2,李晓刚2
(1河海大学力学与材料学院,2北京科技大学新材料技术研究院)
(1河海大学力学与材料学院,2北京科技大学新材料技术研究院)
摘要:本文主要综述了目前我国城市供水管网现状和供水管网的腐蚀现状以及腐蚀过程中存在的一些主要影响因素,同时探讨了供水管网的腐蚀与自来水水质之间的相互关联,为更好的提高城市自来水水质提供参考。
The corrosion status of China's urban water supply pipeline and its influence on water quality
The corrosion status of China's urban water supply pipeline and its influence on water quality
Luo hong1, Liu zhiyong2, Lu Lin2, Dong chaofang2, Li xiaogang2
1College of Mechanics and Materials, Hohai University, Nanjing 210098, China
2Institute of Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083,China
1College of Mechanics and Materials, Hohai University, Nanjing 210098, China
2Institute of Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083,China
Abstract: In this paper, the present status of the urban water supply network in China is reviewed, the corrosion status of water supply network and the main influence factors during the corrosion processes are also displayed. In addition, the correlation between the corrosion of pipeline and the safety of drinking water are discussed, in order to provide reference to improve city water quality better.
联系方式
责任编辑:赵泽南
《中国腐蚀与防护网电子月刊》征订启事
投稿联系:刘娟 电话:010-82387968-807
QQ: 2850329508 邮箱:liujuan@ecorr.org
中国腐蚀与防护网官方 QQ群:140808414
相关文章
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62313558-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
铝合金LDH自修复自抗菌膜层构建
点击数:2727
碳钢及合金钢应用与区别
点击数:2609