08:30-09:00
|
KEYNOTE TALK: Classifications of different biocorrosion types with practical applications in corrosion analysis
|
Ohio University, USA
|
Tingyue Gu
|
|
09:00-09:30
|
KEYNOTE TALK: Laboratory investigation of microbiologically influenced corrosion (mic) resistance of a novel cu-bearing 2205 duplex stainless steel in the presence of aerobic marine pseudomonas aeruginosa biofilm
|
Institute of Metal Research, Chinese Academy of Sciences.
|
Dake Xu
|
|
09:30-09:50
|
Fabrication of slippery liquid-infused porous surface for inhibition of microbially influenced corrosion
|
Institute of Oceanology, Chinese Academy of Sciences (IOCAS),
|
Peng Wang
|
|
09:50-10:10
|
Effect of Pseudomonas on the degradation of coating in seawater
|
Hainan University
|
Ke Chai
|
|
10:10-10:30
|
Selective and specific detection of sulfate-reducing bacteria using potentiometric stripping analysis
|
Institute of Oceanology, Chinese Academy of Sciences
|
Yi Wan
|
|
10:30-10:45
|
茶 歇/Tea Break
|
||
|
10:45-11:05
|
A novel Cu-bearing pipeline steel for microbiologically induced corrosion control
|
Institute of Metal Research, Chinese Academy of Sciences,
|
Xianbo Shi
|
|
11:05-11:25
|
Synthesis of hydrophobic Mg-Al layered double hydroxide film on al with enhanced antifouling performance
|
Institute of Oceanology, Chinese Academy of Sciences
|
Yi Wang
|
|
11:25-11:50
|
The applicability of different electrochemical testing technologys in the study of microbial corrosion research
|
Harbin Engineering University
|
Yuzhi Liu
|
|
12:00-13:30自助午餐
|
|||
时间地点:8月11日上午,丽正厅
分会场主席:徐大可
个人简介

徐大可副研究员
徐大可,中国科学院金属研究所副研究员,2014年获得“中国科学院金属研究所所引进优秀学者”。从事材料微生物腐蚀的机理与防治、抗菌不锈钢抗菌机理的相关研究。毕业于美国俄亥俄大学化学工程系腐蚀与多相流技术中心,曾在NACE 2011 Houston获学生Harvey Herro二等奖。已负责973专项服务课题、国家自然科学基金及企业委托项目共9项。在微生物腐蚀机理及防治相关研究积累了比较丰富的经验,以第一作者或通讯作者发表论文30余篇,获得国际PCT专利1项。
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
-
标签: 徐大可, 2016第四届国际腐蚀工程大会分会主席, 微生物腐蚀和生物污损
相关文章
无相关信息
官方微信
《腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62316606
- 邮箱:fsfhzy666@163.com
- 腐蚀与防护网官方QQ群:140808415
点击排行
PPT新闻
“海洋金属”——钛合金在舰船的
点击数:12773
腐蚀与“海上丝绸之路”
点击数:10744