热烈祝贺! 11月14日,科睿唯安(Clarivate Analytics)公布了2024年11月的ESI最新数据(数据覆盖时间范围为2014年1月至2024年8月),Journal of Materials Science & Technology(JMST)入选ESI高被引论文 167 篇,热点论文 12 篇。 ESI高被引论文: 基于对应领域和出版年的高被引阈值,其被引频次已进入学术领域最优秀的 1% 之列。 ESI热点论文:在过去两年内发表,且在近2个月内被引频次位列学术领域最优秀的 0.1% 之列。
2024年11月ESI高被引论文
1. Microstructure and Fracture Behavior of 316L Austenitic Stainless Steel Produced by Selective Laser Melting
R. Casati, J. Lemke, M. Vedani
J. Mater. Sci. Technol. 32 (2016) 738-744
https://doi.org/10.1016/j.jmst.2016.06.016
2. A Review on Casting Magnesium Alloys: Modification of Commercial Alloys and Development of New Alloys
Fusheng Pan, Mingbo Yang, Xianhua Chen
J. Mater. Sci. Technol. 32 (2016) 1211-1221
https://doi.org/10.1016/j.jmst.2016.07.001
3. Friction stir based welding and processing technologies-processes, parameters, microstructures and applications: A review
G.K. Padhy, C.S. Wu, S. Gao
J. Mater. Sci. Technol. 34 (2018) 1-38
https://doi.org/10.1016/j.jmst.2017.11.029
4. What is going on in magnesium alloys?
X.J. Wang, D.K. Xu, R.Z. Wu, X.B. Chen, Q.M. Peng, L. Jin, Y.C. Xin, Z.Q. Zhang, Y. Liu, X.H. Chen, G. Chen, K.K. Deng, H.Y. Wang
J. Mater. Sci. Technol. 34 (2018) 245-247
https://doi.org/10.1016/j.jmst.2017.07.019
5. Hall-Petch relationship in Mg alloys: A review
Huihui Yu, Yunchang Xin, Maoyin Wang, Qing Liu
J. Mater. Sci. Technol. 34 (2018) 248-256
https://doi.org/10.1016/j.jmst.2017.07.022
6. Anaerobic microbiologically influenced corrosion mechanisms interpreted using bioenergetics and bioelectrochemistry: A review
Yingchao Li, Dake Xu, Changfeng Chen, Xiaogang Li, Ru Jia, Dawei Zhang, Wolfgang Sand, Fuhui Wang, Tingyue Gu
J. Mater. Sci. Technol. 34 (2018) 1713-1718
https://doi.org/10.1016/j.jmst.2018.02.023
7. Progress in additive manufacturing on new materials: A review
Neng Li, Shuai Huang, Guodong Zhang, Renyao Qin, Wei Liu, Huaping Xiong, Gongqi Shi, Jon Blackburn
J. Mater. Sci. Technol. 35 (2019) 242-269
https://doi.org/10.1016/j.jmst.2018.09.002
8. A review of selective laser melting of aluminum alloys: Processing, microstructure, property and developing trends
Jinliang Zhang, Bo Song, Qingsong Wei, Dave Bourell, Yusheng Shi
J. Mater. Sci. Technol. 35 (2019) 270-284
https://doi.org/10.1016/j.jmst.2018.09.004
9. A promising new class of irradiation tolerant materials: Ti2ZrHfV0.5Mo0.2 high-entropy alloy
Yiping Lu, Hefei Huang, Xuzhou Gao, Cuilan Ren, Jie Gao, Huanzhi Zhang, Shijian Zheng, Qianqian Jin, Yonghao Zhao, Chenyang Lu, Tongmin Wang, Tingju Li
J. Mater. Sci. Technol. 35 (2019) 369-373
https://doi.org/10.1016/j.jmst.2018.09.034
10. Toward a better understanding of microbiologically influenced corrosion caused by sulfate reducing bacteria
Tingyue Gu, Ru Jia, Tuba Unsal, Dake Xu
J. Mater. Sci. Technol. 35 (2019) 631-636
https://doi.org/10.1016/j.jmst.2018.10.026
11. Advances on strategies for searching for next generation thermal barrier coating materials
Bin Liu, Yuchen Liu, Changhua Zhu, Huimin Xiang, Hongfei Chen, Luchao Sun, Yanfeng Gao, Yanchun Zhou
J. Mater. Sci. Technol. 35 (2019) 833-851
https://doi.org/10.1016/j.jmst.2018.11.016
12. Mechanical properties and corrosion behavior of selective laser melted 316L stainless steel after different heat treatment processes
Decheng Kong, Chaofang Dong, Xiaoqing Ni, Liang Zhang, Jizheng Yao, Cheng Man, Xuequn Cheng, Kui Xiao, Xiaogang Li
J. Mater. Sci. Technol. 35 (2019) 1499-1507
https://doi.org/10.1016/j.jmst.2019.03.003
13. (La0.2Ce0.2Nd0.2Sm0.2Eu0.2)2Zr2O7: A novel high-entropy ceramic with low thermal conductivity and sluggish grain growth rate
Zifan Zhao, Huimin Xiang, Fu-Zhi Dai, Zhijian Peng, Yanchun Zhou
J. Mater. Sci. Technol. 35 (2019) 2647-2651
https://doi.org/10.1016/j.jmst.2019.05.054
14. Sulfur-doped g-C3N4/rGO porous nanosheets for highly efficient photocatalytic degradation of refractory contaminants
Yanmei Zheng, Yuanyuan Liu, Xinli Guo, Zhongtao Chen, Weijie Zhang, Yixuan Wang, Xuan Tang, Yao Zhang, Yuhong Zhao
J. Mater. Sci. Technol. 41 (2020) 117-126
https://doi.org/10.1016/j.jmst.2019.09.018
15. Progress in achieving high-performance piezoresistive and capacitive flexible pressure sensors: A review
Wufan Chen, Xin Yan
J. Mater. Sci. Technol. 43 (2020) 175-188
https://doi.org/10.1016/j.jmst.2019.11.010
16. Thermodynamics and kinetics of phase transformation in rare earth–magnesium alloys: A critical review
Qun Luo, Yanlin Guo, Bin Liu, Yujun Feng, Jieyu Zhang, Qian Li, Kuochih Chou
J. Mater. Sci. Technol. 44 (2020) 171-190
https://doi.org/10.1016/j.jmst.2020.01.022
17. Self-assembling anchored film basing on two tetrazole derivatives for application to protect copper in sulfuric acid environment
Yujie Qiang, Hao Li, Xijian Lan
J. Mater. Sci. Technol. 52 (2020) 63-71
https://doi.org/10.1016/j.jmst.2020.04.005
18. Lightweight and robust rGO/sugarcane derived hybrid carbon foams with outstanding EMI shielding performance
Lei Wang, Xuetao Shi, Junliang Zhang, Yali Zhang, Junwei Gu
J. Mater. Sci. Technol. 52 (2020) 119-126
https://doi.org/10.1016/j.jmst.2020.03.029
19. MXene-based photocatalysts
Panyong Kuang, Jingxiang Low, Bei Cheng, Jiaguo Yu, Jiajie Fan
J. Mater. Sci. Technol. 56 (2020) 18-44
https://doi.org/10.1016/j.jmst.2020.02.037
20. Recent advances in g-C3N4-based heterojunction photocatalysts
Yunfeng Li, Minghua Zhou, Bei Cheng, Yan Shao
J. Mater. Sci. Technol. 56 (2020) 1-17
https://doi.org/10.1016/j.jmst.2020.04.028
21. BiVO4, Bi2WO6 and Bi2MoO6 photocatalysis: A brief review
Xintong Liu, Shaonan Gu, Yanjun Zhao, Guowei Zhou, Wenjun Li
J. Mater. Sci. Technol. 56 (2020) 45-68
https://doi.org/10.1016/j.jmst.2020.04.023
22. A review on 2D MoS2 cocatalysts in photocatalytic H2 production
Zizhan Liang, Rongchen Shen, Yun Hau Ng, Peng Zhang, Quanjun Xiang, Xin Li
J. Mater. Sci. Technol. 56 (2020) 89-121
https://doi.org/10.1016/j.jmst.2020.04.032
23. Step-scheme CdS/TiO2 nanocomposite hollow microsphere with enhanced photocatalytic CO2 reduction activity
Zhongliao Wang, Yifan Chen, Liuyang Zhang, Bei Cheng, Jiaguo Yu, Jiajie Fan
J. Mater. Sci. Technol. 56 (2020) 143-150
https://doi.org/10.1016/j.jmst.2020.02.062
24. Recent advances on environmental corrosion behavior and mechanism of high-entropy alloys
Yu Fu, Jun Li, Hong Luo, Cuiwei Du, Xiaogang Li
J. Mater. Sci. Technol. 80 (2021) 217-233
https://doi.org/10.1016/j.jmst.2020.11.044
25. Short-range ordering and its effects on mechanical properties of high-entropy alloys
Yuan Wu, Fei Zhang, Xiaoyuan Yuan, Hailong Huang, Xiaocan Wen, Yihan Wang, Mengyuan Zhang, Honghui Wu, Xiongjun Liu, Hui Wang, Suihe Jiang, Zhaoping Lu
J. Mater. Sci. Technol. 62 (2021) 214-220
https://doi.org/10.1016/j.jmst.2020.06.018
26. Improvement of thermal conductivities and simulation model for glass fabrics reinforced epoxy laminated composites via introducing hetero-structured BNN-30@BNNS fillers
Xuetao Shi, Ruihan Zhang, Kunpeng Ruan, Tengbo Ma, Yongqiang Guo, Junwei Gu
J. Mater. Sci. Technol. 82 (2021) 239-249
https://doi.org/10.1016/j.jmst.2021.01.018
27. Investigation on microstructure and mechanical properties of Al-Zn-Mg-Cu alloys with various Zn/Mg ratios
Yan Zou, Xiaodong Wu, Songbai Tang, Qianqian Zhu, Hui Song, Mingxing Guo, Lingfei Cao
J. Mater. Sci. Technol. 85 (2021) 106-117
https://doi.org/10.1016/j.jmst.2020.12.045
28. A review on carbon/magnetic metal composites for microwave absorption
Baolei Wang, Qian Wu, Yonggang Fu, Tong Liu
J. Mater. Sci. Technol. 86 (2021) 91-109
https://doi.org/10.1016/j.jmst.2020.12.078
29. Multifunctional HDPE/CNTs/PW composite phase change materials with excellent thermal and electrical conductivities
Xiaolong Li, Xinxin Sheng, Yongqiang Guo, Xiang Lu, Hao Wu, Ying Chen, Li Zhang, Junwei Gu
J. Mater. Sci. Technol. 86 (2021) 171-179
https://doi.org/10.1016/j.jmst.2021.02.009
30. Heterostructure design of Fe3N alloy/porous carbon nanosheet composites for efficient microwave attenuation
Weihua Gu, Xiaoqing Cui, Jing Zheng, Jiwen Yu, Yue Zhao, Guangbin Ji
J. Mater. Sci. Technol. 67 (2021) 265-272
https://doi.org/10.1016/j.jmst.2020.06.054
31. MOFs derived magnetic porous carbon microspheres constructed by core-shell Ni@C with high-performance microwave absorption
Sai Gao, Guozheng Zhang, Yi Wang, Xiaopeng Han, Ying Huang, Panbo Liu
J. Mater. Sci. Technol. 88 (2021) 56-65
https://doi.org/10.1016/j.jmst.2021.02.011
32. Controllable synthesis of Ni/NiO@porous carbon hybrid composites towards remarkable electromagnetic wave absorption and wide absorption bandwidth
Xinfeng Zhou, Zirui Jia, Xingxue Zhang, Bingbing Wang, Wei Wu, Xuehua Liu, Binghui Xu, Guanglei Wu
J. Mater. Sci. Technol. 87 (2021) 120-132
https://doi.org/10.1016/j.jmst.2021.01.073
33. Hierarchical composite of biomass derived magnetic carbon framework and phytic acid doped polyanilne with prominent electromagnetic wave absorption capacity
Tianqi Hou, Zirui Jia, Ailing Feng, Zehua Zhou, Xuehua Liu, Hualiang Lv, Guanglei Wu
J. Mater. Sci. Technol. 68 (2021) 61-69
https://doi.org/10.1016/j.jmst.2020.06.046
34. Intrinsic high thermal conductive liquid crystal epoxy film simultaneously combining with excellent intrinsic self-healing performance
Xutong Yang, Xiao Zhong, Junliang Zhang, Junwei Gu
J. Mater. Sci. Technol. 68 (2021) 209-215
https://doi.org/10.1016/j.jmst.2020.08.027
35. Polymer matrix wave-transparent composites: A review
Lin Tang, Junliang Zhang, Yusheng Tang, Jie Kong, Tianxi Liu, Junwei Gu
J. Mater. Sci. Technol. 75 (2021) 225-251
https://doi.org/10.1016/j.jmst.2020.09.017
36. Additive manufacturing of high entropy alloys: A practical review
Ahmad Ostovari Moghaddam, Nataliya A. Shaburova, Marina N. Samodurova, Amin Abdollahzadeh, Evgeny A. Trofimov
J. Mater. Sci. Technol. 77 (2021) 131-162
https://doi.org/10.1016/j.jmst.2020.11.029
37. A review: Synthesis, modification and photocatalytic applications of ZnIn2S4
Jie Wang, Sijia Sun, Run Zhou, Yangzi Li, Zetian He, Hao Ding, Daimei Chen, Weihua Ao
J. Mater. Sci. Technol. 78 (2021) 1-19
https://doi.org/10.1016/j.jmst.2020.09.045
38. Green building materials lit up by electromagnetic absorption function: A review
Ting-Ting Liu, Mao-Qing Cao, Yong-Sheng Fang, Yu-Hang Zhu, Mao-Sheng Cao
J. Mater. Sci. Technol. 112 (2022) 329-344
https://doi.org/10.1016/j.jmst.2021.10.022
39. Synergistic regulation of dielectric-magnetic dual-loss and triple heterointerface polarization via magnetic MXene for high-performance electromagnetic wave absorption
Chunhua Sun, Zirui Jia, Shuang Xu, Dongqi Hu, Chuanhui Zhang, Guanglei Wu
J. Mater. Sci. Technol. 113 (2021) 128-137
https://doi.org/10.1016/j.jmst.2021.11.006
40. Design, Preparation and Properties of Carbon Fiber Reinforced Ultra-High Temperature Ceramic Composites for Aerospace Applications: A Review
Sufang Tang, Chenglong Hu
J. Mater. Sci. Technol. 33 (2017) 117-130
https://doi.org/10.1016/j.jmst.2016.08.004
41. Silicone/graphene oxide co-cross-linked aerogels with wide-temperature mechanical flexibility, super-hydrophobicity and flame resistance for exceptional thermal insulation and oil/water separation
Zhao-Hui Zhang, Zuan-Yu Chen, Yi-Hao Tang, Yu-Tong Li, Dequan Ma, Guo-Dong Zhang, Rabah Boukherroub, Cheng-Fei Cao, Li-Xiu Gong, Pingan Song, Kun Cao, Long-Cheng Tang
J. Mater. Sci. Technol. 114 (2022) 131-142
https://doi.org/10.1016/j.jmst.2021.11.012
42. Enhanced photocatalytic degradation and H2 evolution performance of NCDs/S-C3N4 S-scheme heterojunction constructed by π-π conjugate self-assembly
Xibao Li, Qiuning Luo, Lu Han, Fang Deng, Ya Yang, Fan Dong
J. Mater. Sci. Technol. 114 (2022) 222-232
https://doi.org/10.1016/j.jmst.2021.10.030
43. Oxygen vacancies induced narrow band gap of BiOCl for efficient visible-light catalytic performance from double radicals
Changyan Chen, Ting Jiang, Jianhua Hou, Tingting Zhang, Geshan Zhang, Yongcai Zhang, Xiaozhi Wang
J. Mater. Sci. Technol. 114 (2022) 240-248
https://doi.org/10.1016/j.jmst.2021.12.006
44. Structure characteristics and microwave dielectric properties of Pr2(Zr1−xTix)3(MoO4)9 solid solution ceramic with a stable temperature coefficient
Huanrong Tian, Jinjie Zheng, Lintao Liu, Haitao Wu, Hideo Kimura, Yizhong Lu, Zhenxing Yue
J. Mater. Sci. Technol. 116 (2022) 121-129
https://doi.org/10.1016/j.jmst.2021.10.051
45. Active anticorrosion and self-healing coatings: A review with focus on multi-action smart coating strategies
Inime Ime Udoh, Hongwei Shi, Enobong Felix Daniel, Jianyang Li, Songhua Gu, Fuchun Liu, En-Hou Han
J. Mater. Sci. Technol. 116 (2022) 224-237
https://doi.org/10.1016/j.jmst.2021.11.042
46. In-situ fabrication of Bi2S3/BiVO4/Mn0.5Cd0.5S-DETA ternary S-scheme heterostructure with effective interface charge separation and CO2 reduction performance
Zhiwei Zhao, Xiaofeng Li, Kai Dai, Jinfeng Zhang, Graham Dawson
J. Mater. Sci. Technol. 117 (2022) 109-119
https://doi.org/10.1016/j.jmst.2021.11.046
47. Additive manufacturing of metals: Microstructure evolution and multistage control
Zhiyuan Liu, Dandan Zhao, Pei Wang, Ming Yan, Can Yang, Zhangwei Chen, Jian Lu, Zhaoping Lu
J. Mater. Sci. Technol. 100 (2022) 224-236
https://doi.org/10.1016/j.jmst.2021.06.011
48. Sulfur-doped g-C3N4/g-C3N4 isotype step-scheme heterojunction for photocatalytic H2 evolution
Jizhou Jiang, Zhiguo Xiong, Haitao Wang, Guodong Liao, Saishuai Bai, Jing Zou, Pingxiu Wu, Peng Zhang, Xin Li
J. Mater. Sci. Technol. 118 (2022) 15-24
https://doi.org/10.1016/j.jmst.2021.12.018
49. Mixed-dimensional hierarchical configuration of 2D Ni2P nanosheets anchored on 1D silk-derived carbon fiber for extraordinary electromagnetic wave absorption
Fei Pan, Lei Cai, Yanyan Dong, Xiaojie Zhu, Yuyang Shi, Wei Lu
J. Mater. Sci. Technol. 101 (2022) 85-94
https://doi.org/10.1016/j.jmst.2021.05.066
50. Surface decoration of Halloysite nanotubes with POSS for fire-safe thermoplastic polyurethane nanocomposites
Wei Wu, Wanjing Zhao, Xianjing Gong, Qijun Sun, Xianwu Cao, Yujun Su, Bin Yu, Robert K.Y. Li, Roy A.L. Vellaisamy
J. Mater. Sci. Technol. 101 (2022) 107-117
https://doi.org/10.1016/j.jmst.2021.05.060
51. Simultaneous enhancement of mechanical and shape memory properties by heat-treatment homogenization of Ti2Ni precipitates in TiNi shape memory alloy fabricated by selective laser melting
H.Z. Lu, L.H. Liu, C. Yang, X. Luo, C.H. Song, Z. Wang, J. Wang, Y.D. Su, Y.F. Ding, L.C. Zhang, Y.Y. Li
J. Mater. Sci. Technol. 101 (2022) 205-216
https://doi.org/10.1016/j.jmst.2021.06.019
52. Micro-arc oxidation of magnesium alloys: A review
Wenhui Yao, Liang Wu, Jingfeng Wang, Bin Jiang, Dingfei Zhang, Maria Serdechnova, Tatsiana Shulha, Carsten Blawert, Mikhail L. Zheludkevich, Fusheng Pan
J. Mater. Sci. Technol. 118 (2022) 158-180
https://doi.org/10.1016/j.jmst.2021.11.053
53. Achievement of giant cryogenic refrigerant capacity in quinary rare-earths based high-entropy amorphous alloy
Yikun Zhang, Jian Zhu, Shuo Li, Jiang Wang, Zhongming Ren
J. Mater. Sci. Technol. 102 (2022) 66-71
https://doi.org/10.1016/j.jmst.2021.06.028
54. Refinement mechanism of cerium addition on solidification structure and sigma phase of super austenitic stainless steel S32654
Shucai Zhang, Jiangtao Yu, Huabing Li, Zhouhua Jiang, Yifeng Geng, Hao Feng, Binbin Zhang, Hongchun Zhu
J. Mater. Sci. Technol. 102 (2022) 105-114
https://doi.org/10.1016/j.jmst.2021.06.033
55. Layered double hydroxide (LDH) for multi-functionalized corrosion protection of metals: A review
Yanhui Cao, Dajiang Zheng, Fan Zhang, Jinshan Pan, Changjian Lin
J. Mater. Sci. Technol. 102 (2022)
https://doi.org/10.1016/j.jmst.2021.05.078
56. An advanced cathode composite for co-utilization of cations and anions in lithium batteries
Xiao-Tong Wang, Yang Yang, Jin-Zhi Guo, Zhen-Yi Gu, Edison Huixiang Ang, Zhong-Hui Sun, Wen-Hao Li, Hao-Jie Liang, Xing-Long Wu
J. Mater. Sci. Technol. (2022) 72-79
https://doi.org/10.1016/j.jmst.2021.05.074
57. Photoinduced self-stability mechanism of CdS photocatalyst: The dependence of photocorrosion and H2-evolution performance
Yuxiao Chen, Wei Zhong, Feng Chen, Ping Wang, Jiajie Fan, Huogen Yu
J. Mater. Sci. Technol. 121 (2022) 19-27
https://doi.org/10.1016/j.jmst.2021.12.051
58. EDA-assisted synthesis of multifunctional snowflake-Cu2S/CdZnS S-scheme heterojunction for improved the photocatalytic hydrogen evolution
Guorong Wang, Yongkang Quan, Kaicheng Yang, Zhiliang Jin
J. Mater. Sci. Technol. 121 (2022) 28-39
https://doi.org/10.1016/j.jmst.2021.11.073
59. Porous carbon polyhedrons coupled with bimetallic CoNi alloys for frequency selective wave absorption at ultralow filler loading
Yan-Li Wang, Guang-Sheng Wang, Xiao-Juan Zhang, Chen Gao
J. Mater. Sci. Technol. 103 (2022) 28-39
https://doi.org/10.1016/j.jmst.2021.11.073
60. A mini-review of MXene porous films: Preparation, mechanism and application
Yali Zhang, Yi Yan, Hua Qiu, Zhonglei Ma, Kunpeng Ruan, Junwei Gu
J. Mater. Sci. Technol. 103 (2022) 34-41
https://doi.org/10.1016/j.jmst.2021.06.021
61. Synthesis of MnxOy@C hybrid composites for optimal electromagnetic wave absorption capacity and wideband absorption
Yue Liu, Xuehua Liu, Xinyu E, Bingbing Wang, Zirui Jia, Qingguo Chi, Guanglei Wu
J. Mater. Sci. Technol. 103 (2022) 157-164
https://doi.org/10.1016/j.jmst.2021.06.034
62. Multi-scale defects in powder-based additively manufactured metals and alloys
J. Fu, H. Li, X. Song, M.W. Fu,
J. Mater. Sci. Technol. 122 (2022) 165-199
https://doi.org/10.1016/j.jmst.2022.02.015
63. N-doped residual carbon from coal gasification fine slag decorated with Fe3O4 nanoparticles for electromagnetic wave absorption
Jun He, Shengtao Gao, Yuanchun Zhang, Xingzhao Zhang, Hanxu Li
J. Mater. Sci. Technol. 104 (2022) 98-108
https://doi.org/10.1016/j.jmst.2021.06.052
64. Metal sulfides based composites as promising efficient microwave absorption materials: A review
Bin Li, Fenglong Wang, Kejun Wang, Jing Qiao, Dongmei Xu, Yunfei Yang, Xue Zhang, Longfei Lyu, Wei Liu, Jiurong Liu
J. Mater. Sci. Technol. 104 (2022) 244-268
https://doi.org/10.1016/j.jmst.2021.06.065
65. ZnWO4-ZnIn2S4 S-scheme heterojunction for enhanced photocatalytic H2 evolution
Meng Dai, Zuoli He, Peng Zhang, Xin Li, Shuguang Wang
J. Mater. Sci. Technol. 122 (2022) 231-242
https://doi.org/10.1016/j.jmst.2022.02.014
66. Rationally designed Ta3N5/BiOCl S-scheme heterojunction with oxygen vacancies for elimination of tetracycline antibiotic and Cr(VI): Performance, toxicity evaluation and mechanism insight
Shijie Li, Mingjie Cai, Chunchun Wang, Yanping Liu, Neng Li, Peng Zhang, Xin Li
J. Mater. Sci. Technol. 123 (2022) 177-190
https://doi.org/10.1016/j.jmst.2022.02.012
67. Sonochemical synthesis of photocatalysts and their applications
Kezhen Qi, Chunqiang Zhuang, Manjie Zhang, Peyman Gholami, Alireza Khataee
J. Mater. Sci. Technol. 123 (2022) 243-256
https://doi.org/10.1016/j.jmst.2022.02.019
68. Improved electromagnetic dissipation of Fe doping LaCoO3 toward broadband microwave absorption
Fan Wang, Weihua Gu, Jiabin Chen, Qianqian Huang, Mingyang Han, Gehuan Wang, Guangbin Ji
J. Mater. Sci. Technol. 105 (2022) 92-100
https://doi.org/10.1016/j.jmst.2021.06.058
69. Switch type PANI/ZnO core-shell microwire heterojunction for UV photodetection
Yihan Chen, Longxing Su, Mingming Jiang, Xiaosheng Fang
J. Mater. Sci. Technol. 105 (2022) 259-265
https://doi.org/10.1016/j.jmst.2021.07.031
70. S-scheme CoTiO3/ Cd9.51Zn0.49S10 heterostructures for visible-light driven photocatalytic CO2 reduction
Bo Su, Haowei Huang, Zhengxin Ding, Maarten B.J. Roeffaers, Sibo Wang, Jinlin Long
J. Mater. Sci. Technol. 124 (2022) 164-170
https://doi.org/10.1016/j.jmst.2022.01.030
71. Design principle of S-scheme heterojunction photocatalyst
Quanlong Xu, S. Wageh, Ahmed A. Al-Ghamdi, Xin Li
J. Mater. Sci. Technol. 124 (2022) 171-173
https://doi.org/10.1016/j.jmst.2022.02.016
72. S-scheme ZnO/WO3 heterojunction photocatalyst for efficient H2O2 production
Zicong Jiang, Bei Cheng, Yong Zhang, S. Wageh, Ahmed A. Al‐Ghamdi, Jiaguo Yu, Linxi Wang
J. Mater. Sci. Technol. 124 (2022) 193-201
https://doi.org/10.1016/j.jmst.2022.01.029
73. Review on g-C3N4-based S-scheme heterojunction photocatalysts
Yunfeng Li, Zhiling Xia, Qing Yang, Linxi Wang, Yan Xing
J. Mater. Sci. Technol. 125 (2022) 128-144
https://doi.org/10.1016/j.jmst.2022.02.035
74. Highly transmitted silver nanowires-SWCNTs conductive flexible film by nested density structure and aluminum-doped zinc oxide capping layer for flexible amorphous silicon solar cells
Shunliang Gao, Xiaohui Zhao, Qi Fu, Tianchi Zhang, Jun Zhu, Fuhua Hou, Jian Ni, Chengjun Zhu, Tiantian Li, Yanlai Wang, Vignesh Murugadoss, Gaber A.M. Mersal, Mohamed M. Ibrahim, Zeinhom M. El-Bahy, Mina Huang, Zhanhu Guo
J. Mater. Sci. Technol. 126 (2022) 152-160
https://doi.org/10.1016/j.jmst.2022.03.012
75. High-performance microwave absorption enabled by Co3O4 modified VB-group laminated VS2 with frequency modulation from S-band to Ku-band
Zehao Huang, Junye Cheng, Huibin Zhang, Yingfei Xiong, Zhanxin Zhou, Qingbin Zheng, Guangping Zheng, Deqing Zhang, Maosheng Cao
J. Mater. Sci. Technol. 107 (2022) 155-164
https://doi.org/10.1016/j.jmst.2021.08.005
76. Regulating bifunctional flower-like NiFe2O4/graphene for green EMI shielding and lithium ion storage
Lihua Yao, Wenqiang Cao, Jianguo Zhao, Qi Zheng, Yuchang Wang, Shang Jiang, Qiliang Pan, Jie Song, Youqi Zhu, Maosheng Cao
J. Mater. Sci. Technol. 127 (2022) 48-60
https://doi.org/10.1016/j.jmst.2022.04.010
77. Hierarchical red phosphorus incorporated TiO2 hollow sphere heterojunctions toward superior photocatalytic hydrogen production
Guiqing Huang, Wanneng Ye, Chunxiao Lv, Denys S. Butenko, Chen Yang, Gaolian Zhang, Ping Lu, Yan Xu, Shuchao Zhang, Hongwei Wang, Yukun Zhu, Dongjiang Yang
J. Mater. Sci. Technol. 108 (2022) 18-25
https://doi.org/10.1016/j.jmst.2021.09.026
78. Magnetic NiFe2O4/Polypyrrole nanocomposites with enhanced electromagnetic wave absorption
Jiang Guo, Xu Li, Zhuoran Chen, Jianfeng Zhu, Xianmin Mai, Renbo Wei, Kai Sun, Hu Liu, Yunxia Chen, Nithesh Naik, Zhanhu Guo
J. Mater. Sci. Technol. 108 (2022) 64-72
https://doi.org/10.1016/j.jmst.2021.08.049
79. Tunable Co/ZnO/C@MWCNTs based on carbon nanotube-coated MOF with excellent microwave absorption properties
Zirui Jia, Mingyue Kong, Bowen Yu, Yingzhuo Ma, Jiaying Pan, Guanglei Wu
J. Mater. Sci. Technol. 127 (2022) 153-163
https://doi.org/10.1016/j.jmst.2022.04.005
80. Microstructure optimization of core@shell structured MSe2/FeSe2@MoSe2 (M = Co, Ni) flower-like multicomponent nanocomposites towards high-efficiency microwave absorption
Jingjing Zhang, Xiaosi Qi, Xiu Gong, Qiong Peng, Yanli Chen, Ren Xie, Wei Zhong
J. Mater. Sci. Technol. 128 (2022) 59-70
https://doi.org/10.1016/j.jmst.2022.04.017
81. Heterostructure design of MOFs derived Co9S8/FeCoS2/C composite with efficient microwave absorption and waterproof functions
Runrun Cheng, Yan Wang, Xiaochuang Di, Zhao Lu, Ping Wang, Xinming Wu
J. Mater. Sci. Technol. 129 (2022) 15-26
https://doi.org/10.1016/j.jmst.2022.04.031
82. Trimetallic oxyhydroxides as active sites for large-current-density alkaline oxygen evolution and overall water splitting
Lei Chen, Yunpeng Wang, Xin Zhao, Yuchao Wang, Qian Li, Qichen Wang, Yougen Tang, Yongpeng Lei
J. Mater. Sci. Technol. 110 (2022) 128-135
https://doi.org/10.1016/j.jmst.2021.08.083
83. Ultrastrong and ductile BCC high-entropy alloys with low-density via dislocation regulation and nanoprecipitates
Xuehui Yan, Peter K. Liaw, Yong Zhang
J. Mater. Sci. Technol. 110 (2022) 109-116
https://doi.org/10.1016/j.jmst.2021.08.034
84. Unique strength-ductility balance of AlCoCrFeNi2.1 eutectic high entropy alloy with ultra-fine duplex microstructure prepared by selective laser melting
Yinuo Guo, Haijun Su, Haotian Zhou, Zhonglin Shen, Yuan Liu, Jun Zhang, Lin Liu, Hengzhi Fu
J. Mater. Sci. Technol. 111 (2022) 298-306
https://doi.org/10.1016/j.jmst.2021.10.013
85. Solar fuel generation over nature-inspired recyclable TiO2/g-C3N4 S-scheme hierarchical thin-film photocatalyst
Libo Wang, Xingang Fei, Liuyang Zhang, Jiaguo Yu, Bei Cheng, Yuhua Ma
J. Mater. Sci. Technol. 112 (2022) 1-10
https://doi.org/10.1016/j.jmst.2021.10.016
86. Regulating interfacial morphology and charge-carrier utilization of Ti3C2 modified all-sulfide CdS/ZnIn2S4 S-scheme heterojunctions for effective photocatalytic H2 evolution
Junxian Bai, Weilin Chen, Rongchen Shen, Zhimin Jiang, Peng Zhang, Wei Liu, Xin Li
J. Mater. Sci. Technol. 112 (2022) 85-95
https://doi.org/10.1016/j.jmst.2021.11.003
87. Electrochemical measurements used for assessment of corrosion and protection of metallic materials in the field: A critical review
Da-Hai Xia, Cheng-Man Deng, Digby Macdonald, Sina Jamali, Douglas Mills, Jing-Li Luo, Michael G. Strebl, Mehdi Amiri, Weixian Jin, Shizhe Song, Wenbin Hu
J. Mater. Sci. Technol. 112 (2022) 151-181
https://doi.org/10.1016/j.jmst.2021.11.004
88. Superhydrophobic self-extinguishing cotton fabrics for electromagnetic interference shielding and human motion detection
Lei Liu, Zhewen Ma, Menghe Zhu, Lina Liu, Jinfeng Dai, Yongqian Shi, Jiefeng Gao, Toan Dinh, Thanh Nguyen, Long-Cheng Tang, Pingan Song
J. Mater. Sci. Technol. 132 (2023) 59-68
https://doi.org/10.1016/j.jmst.2022.05.036
89. Construction of three-dimensional hierarchical porous nitrogen-doped reduced graphene oxide/hollow cobalt ferrite composite aerogels toward highly efficient electromagnetic wave absorption
Jing Xu, Ruiwen Shu, Zongli Wan, Jianjun Shi
J. Mater. Sci. Technol. 132 (2023) 193-200
https://doi.org/10.1016/j.jmst.2022.05.050
90. Recent progress on multifunctional electromagnetic interference shielding polymer composites
Ke Tian, Danrong Hu, Quan Wei, Qiang Fu, Hua Deng
J. Mater. Sci. Technol. 134 (2023) 106-131
https://doi.org/10.1016/j.jmst.2022.06.031
91. Recent progress in the development of RE2TMTM’O6 double perovskite oxides for cryogenic magnetic refrigeration
Lingwei Li, Mi Yan
J. Mater. Sci. Technol. 136 (2023) 1-12
https://doi.org/10.1016/j.jmst.2022.01.041
92. Rapid self-healing, self-adhesive, anti-freezing, moisturizing, antibacterial and multi-stimuli-responsive PVA/starch/tea polyphenol-based composite conductive organohydrogel as flexible strain sensor
Tao Ke, Li Zhao, Xin Fan, Haibin Gu
J. Mater. Sci. Technol. 135 (2023) 199-212
https://doi.org/10.1016/j.jmst.2022.06.032
93. Boosted lithium storage performance by local build-in electric field derived by oxygen vacancies in 3D holey N-doped carbon structure decorated with molybdenum dioxide
Chuanxin Hou, Wenyue Yang, Hideo Kimura, Xiubo Xie, Xiaoyu Zhang, Xueqin Sun, Zhipeng Yu, Xiaoyang Yang, Yuping Zhang, Bin Wang, Ben Bin Xu, Deepak Sridhar, Hassan Algadi, Zhanhu Guo, Wei Du
J. Mater. Sci. Technol. 142 (2023) 185-195
https://doi.org/10.1016/j.jmst.2022.10.007
94. Refractory high-entropy alloys: A focused review of preparation methods and properties
Wei Xiong, Amy X.Y. Guo, Shuai Zhan, Chain-Tsuan Liu, Shan Cecilia Cao
J. Mater. Sci. Technol. 142 (2023) 196-215
https://doi.org/10.1016/j.jmst.2022.08.046
95. Photocatalysis vs adsorption by metal oxide nanoparticles
Usman Qumar, Jahan Zeb Hassan, Rukhsar Ahmad Bhatti, Ali Raza, Ghazanfar Nazir, Walid Nabgan, Muhammad Ikram
J. Mater. Sci. Technol. 131 (2023) 122-166
https://doi.org/10.1016/j.jmst.2022.05.02096. In-situ observation of microcrack initiation and damage nucleation modes on the HAZ of laser-welded DP1180 joint
Junliang Xue, Wei Guo, Jin Yang, Mingsheng Xia, Guang Zhao, Caiwang Tan, Zhandong Wan, Jiaxuan Chi, Hongqiang Zhang
J. Mater. Sci. Technol. 148 (2023) 138-149
https://doi.org/10.1016/j.jmst.2023.01.001
97. Tuning microwave absorption properties of Ti3C2Tx MXene-based materials: Component optimization and structure modulation
Ming Chang, Qingyu Li, Zirui Jia, Wanru Zhao, Guanglei Wu
J. Mater. Sci. Technol. 148 (2023) 150-170
https://doi.org/10.1016/j.jmst.2022.11.021
98. Enhancing hydrogen storage properties of MgH2 using FeCoNiCrMn high entropy alloy catalysts
Haiyi Wan, Xiu Yang, Shiming Zhou, Lei Ran, Yangfan Lu, Yu'an Chen, Jingfeng Wang, Fusheng Pan
J. Mater. Sci. Technol. 149 (2023) 88-98
https://doi.org/10.1016/j.jmst.2022.11.033
99. Morphology controllable urchin-shaped bimetallic nickel-cobalt oxide/carbon composites with enhanced electromagnetic wave absorption performance
Fushan Li, Qiuyu Li, Hideo Kimura, Xiubo Xie, Xiaoyu Zhang, Nannan Wu, Xueqin Sun, Ben Bin Xu, Hassan Algadi, Rami Adel Pashameah, Abdullah K. Alanazi, Eman Alzahrani, Handong Li, Wei Du, Zhanhu Guo, Chuanxin Hou
J. Mater. Sci. Technol. 148 (2023) 250-259
https://doi.org/10.1016/j.jmst.2022.12.003
100. Light-weight refractory high-entropy alloys: A comprehensive review
Zechun Wang, Shiyao Chen, Shenglan Yang, Qun Luo, Yancheng Jin, Wei Xie, Lijun Zhang, Qian Li
J. Mater. Sci. Technol. 151 (2023) 41-65
https://doi.org/10.1016/j.jmst.2022.11.054
101. Sulphur vacancy defects engineered metal sulfides for amended photo(electro)catalytic water splitting: A review
Kusum Sharma, Abhinandan Kumar, Tansir Ahamad, Quyet Van Le, Pankaj Raizada, Archana Singh, Lan Huong Nguyen, Sourbh Thakur, Van-Huy Nguyen, Pardeep Singh
J. Mater. Sci. Technol. 152 (2023) 50-64
https://doi.org/10.1016/j.jmst.2022.11.053
102. A novel cobalt-free oxide dispersion strengthened medium-entropy alloy with outstanding mechanical properties and irradiation resistance
Ao Fu, Bin Liu, Bo Liu, Yuankui Cao, Jian Wang, Tao Liao, Jia Li, Qihong Fang, Peter K. Liaw, Yong Liu
J. Mater. Sci. Technol. 152 (2023) 190-200
https://doi.org/10.1016/j.jmst.2022.11.061
103. In-suit fabricating an efficient electronic transport channels via S-scheme polyaniline/Cd0.5Zn0.5S heterojunction for rapid removal of tetracycline hydrochloride and hydrogen production
Yan Xiao, Yinhua Jiang, Ershuai Zhou, Wenli Zhang, Yan Liu, Jianming Zhang, Xiangyang Wu, Qi Qi, Zhanchao Liu
J. Mater. Sci. Technol. 153 (2023) 205-218
https://doi.org/10.1016/j.jmst.2022.12.060
104. Graphdiyne (CnH2n-2) based CuI-GDY/ZnAl LDH double S-scheme heterojunction proved with in situ XPS for efficient photocatalytic hydrogen production
Tian Wang, Zhiliang Jin
J. Mater. Sci. Technol. 155 (2023) 132-141
https://doi.org/10.1016/j.jmst.2023.03.002
105. Novel BiOBr/Bi2S3 high-low junction prepared by molten salt method for boosting photocatalytic degradation and H2O2 production
Shishi Shen, Xibao Li, Yingtang Zhou, Lu Han, Yu Xie, Fang Deng, Juntong Huang, Zhi Chen, Zhijun Feng, Jilin Xu, Fan Dong
J. Mater. Sci. Technol. 155 (2023) 148-159
https://doi.org/10.1016/j.jmst.2023.03.006
106. A hierarchical Bi-MOF-derived BiOBr/Mn0.2Cd0.8S S-scheme for visible-light-driven photocatalytic CO2 reduction
Jiahui Hua, Zhongliao Wang, Jinfeng Zhang, Kai Dai, Chunfeng Shao, Ke Fan
J. Mater. Sci. Technol. 156 (2023) 64-71
https://doi.org/10.1016/j.jmst.2023.03.003
107. Oxygen-assisted spinodal structure achieves 1.5 GPa yield strength in a ductile refractory high-entropy alloy
Dingcong Cui, Yuyu Zhang, Linxiang Liu, Yue Li, Lei Wang, Zhijun Wang, Junjie Li, Jincheng Wang, Feng He
J. Mater. Sci. Technol. 157 (2023) 11-20
https://doi.org/10.1016/j.jmst.2023.01.038
108. Synergistic effect of phosphorus doping and MoS2 co-catalysts on g-C3N4 photocatalysts for enhanced solar water splitting
Xunfu Zhou, Pai Wang, Meng Li, Minfu Wu, Bei Jin, Jin Luo, Meifeng Chen, Xiaoqin Zhou, Yanning Zhang, Xiaosong Zhou
J. Mater. Sci. Technol. 158 (2023) 171-179
https://doi.org/10.1016/j.jmst.2023.02.041
109. Carbon nanotubes decorated FeNi/nitrogen-doped carbon composites for lightweight and broadband electromagnetic wave absorption
Hongxia Zhang, Kaige Sun, Kangkang Sun, Lei Chen, Guanglei Wu
J. Mater. Sci. Technol. 158 (2023) 242-252
https://doi.org/10.1016/j.jmst.2023.01.053
110. Core-shell Ni3Sn2@C particles anchored on 3D N-doped porous carbon skeleton for modulated electromagnetic wave absorption
Juhua Luo, Wenxing Yan, Xiaopeng Li, Pengcheng Shu, Jie Mei, Yafan Shi
J. Mater. Sci. Technol. 158 (2023) 207-217
https://doi.org/10.1016/j.jmst.2023.01.051
111. Exploration of the rare-earth cobalt nickel-based magnetocaloric materials for hydrogen liquefaction
Yikun Zhang, Jiayu Ying, Xinqiang Gao, Zhaojun Mo, Jun Shen, Lingwei Li
J. Mater. Sci. Technol. 159 (2023) 163-169
https://doi.org/10.1016/j.jmst.2023.04.001
112. Review on multi-dimensional assembled S-scheme heterojunction photocatalysts
Jiani Lu, Shaonan Gu, Hongda Li, Yinan Wang, Meng Guo, Guowei Zhou
J. Mater. Sci. Technol. 160 (2023) 214-239
https://doi.org/10.1016/j.jmst.2023.03.027
113. Single-atom Cu anchored on N-doped graphene/carbon nitride heterojunction for enhanced photocatalytic H2O2 production
Han Li, Bicheng Zhu, Bei Cheng, Guoqiang Luo, Jingsan Xu, Shaowen Cao
J. Mater. Sci. Technol. 161 (2023) 192-200
https://doi.org/10.1016/j.jmst.2023.03.039
114. 3D ordered macroporous sulfur-doped g-C3N4/TiO2 S-scheme photocatalysts for efficient H2O2 production in pure water
Zicong Jiang, Qing Long, Bei Cheng, Rongan He, Linxi Wang
J. Mater. Sci. Technol. 162 (2023) 1-10
https://doi.org/10.1016/j.jmst.2023.03.045
115. Tailoring S-scheme-based carbon nanotubes (CNTs) mediated Ag-CuBi2O4/Bi2S3 nanomaterials for photocatalytic dyes degradation in the aqueous system
Vishal Dutta, Anita Sudhaik, Sonu, Pankaj Raizada, Archana Singh, Tansir Ahamad, Sourbh Thakur, Quyet Van Le, Van-Huy Nguyen, Pardeep Singh
J. Mater. Sci. Technol. 162 (2023) 11-24
https://doi.org/10.1016/j.jmst.2023.03.037
116. S/N-co-doped graphite nanosheets exfoliated via three-roll milling for high-performance sodium/potassium ion batteries
Xin Wang, Zhicong Luo, Juntong Huang, Zhi Chen, Tong Xiang, Zhijun Feng, Jing Wang, Sinong Wang, Yongcun Ma, Huiyong Yang, Xibao Li
J. Mater. Sci. Technol. 147 (2023) 47-55
https://doi.org/10.1016/j.jmst.2022.11.015
117. Enhancing electromagnetic absorption performance of Molybdate@Carbon by metal ion substitution
Aming Xie, Daohu Sheng, Wenli Liu, Youjian Chen, Siyao Cheng
J. Mater. Sci. Technol. 163 (2023) 92-100
https://doi.org/10.1016/j.jmst.2023.05.004
118. Enhanced antibiotic degradation performance of Cd0.5Zn0.5S/Bi2MoO6 S-scheme photocatalyst by carbon dot modification
Shijie Li, Ruyu Yan, Mingjie Cai, Wei Jiang, Mingyi Zhang, Xin Li
J. Mater. Sci. Technol. 164 (2023) 59-67
https://doi.org/10.1016/j.jmst.2023.05.009
119. Wafer-scale heterogeneous integration of self-powered lead-free metal halide UV photodetectors with ultrahigh stability and homogeneity
Ming Deng, Ziqing Li, Xiaolei Deng, Ying Hu, Xiaosheng Fang
J. Mater. Sci. Technol. 164 (2023) 150-159
https://doi.org/10.1016/j.jmst.2023.05.007
120. Flexible thermoregulatory microcapsule/polyurethane-MXene composite films with multiple thermal management functionalities and excellent EMI shielding performance
Danyuan Huang, Ying Chen, Li Zhang, Xinxin Sheng
J. Mater. Sci. Technol. 165 (2023) 27-38
https://doi.org/10.1016/j.jmst.2023.05.013
121. Review on inorganic-organic S-scheme photocatalysts
Jing Wang, Zhongliao Wang, Kai Dai, Jinfeng Zhang
J. Mater. Sci. Technol. 165 (2023) 187-218
https://doi.org/10.1016/j.jmst.2023.03.067
122. High-performance flexible nanocomposites with superior fire safety and ultra-efficient electromagnetic interference shielding
Miao Liu, Kexin Chen, Yongqian Shi, Hengrui Wang, Shijie Wu, Ruizhe Huang, Yuezhan Feng, Longcheng Tang, Xiaohuan Liu, Pingan Song
J. Mater. Sci. Technol. 166 (2023) 133-144
https://doi.org/10.1016/j.jmst.2023.05.017
123. ZnIn2S4-based S-scheme heterojunction photocatalyst
Xinhe Wu, Guoqiang Chen, Liangting Li, Juan Wang, Guohong Wang
J. Mater. Sci. Technol. 167 (2023) 184-204
https://doi.org/10.1016/j.jmst.2023.05.046
124. S-scheme heterojunction in photocatalytic hydrogen production
Teng Li, Noritatsu Tsubaki, Zhiliang Jin
J. Mater. Sci. Technol. 169 (2024) 82-104
https://doi.org/10.1016/j.jmst.2023.04.049
125. Advancements in S-scheme heterojunction materials for photocatalytic environmental remediation
Changliang Nie, Xiaohan Wang, Ping Lu, Yukun Zhu, Xin Li, Hua Tang
J. Mater. Sci. Technol. 169 (2024) 182-198
https://doi.org/10.1016/j.jmst.2023.06.011
126. CuInS2 quantum-dot-modified g-C3N4 S-scheme heterojunction photocatalyst for hydrogen production and tetracycline degradation
Teng Li, Noritatsu Tsubaki, Zhiliang Jin
J. Mater. Sci. Technol. 172 (2024) 145-155
https://doi.org/10.1016/j.jmst.2023.06.042
127. Pomegranate-like ATO/SiO2 microspheres for efficient microwave absorption in wide temperature spectrum
Zhiyang Jiang, Yanjie Gao, Zhihao Pan, Miaomiao Zhang, Jianhui Guo, Jingwei Zhang, Chunhong Gong
J. Mater. Sci. Technol. 174 (2024) 195-203
https://doi.org/10.1016/j.jmst.2023.08.013
128. Synthesis of nitrogen-doped reduced graphene oxide/magnesium ferrite/polyaniline composite aerogel as a lightweight, broadband and efficient microwave absorber
Ruiwen Shu, Lijuan Nie, Ziwei Zhao, Xunhong Yang
J. Mater. Sci. Technol. 175 (2024) 115-124
https://doi.org/10.1016/j.jmst.2013.08.015
129. Hollow engineering of sandwich NC@Co/NC@MnO2 composites toward strong wideband electromagnetic wave attenuation
Chenhao Wei, Lingzi Shi, Maoqing Li, Mukun He, Mengjie Li, Xinrui Jing, Panbo Liu, Junwei Gu
J. Mater. Sci. Technol. 175 (2024) 194-203
https://doi.org/10.1016/j.jmst.2023.08.020
130. A review of updated S-scheme heterojunction photocatalysts
Fangyi Li, Guihua Zhu, Jizhou Jiang, Lang Yang, Fengxia Deng, Arramel, Xin Li
J. Mater. Sci. Technol. 177 (2024) 142-180
https://doi.org/10.1016/j.jmst.2023.08.038
131. Dual strategy of A-site ion substitution and self-assembled MoS2 wrapping to boost permittivity for reinforced microwave absorption performance
Ailing Feng, Di Lan, Jinkun Liu, Guanglei Wu, Zirui Jia
J. Mater. Sci. Technol. 180 (2024) 1-11
https://doi.org/10.1016/j.jmst.2023.08.060
132. Enhanced photocatalytic performance of S-scheme CdMoO4/CdO nanosphere photocatalyst
Zhe Chen, Tinglin Ma, Zongjun Li, Wenjing Zhu, Lingling Li
J. Mater. Sci. Technol. 179 (2024) 198-207
https://doi.org/10.1016/j.jmst.2023.07.029
133. PEDOT:PSS-patched magnetic graphene films with tunable dielectric genes for electromagnetic interference shielding and infrared stealth
Jin-Cheng Shu, Yu-Ze Wang, Mao-Sheng Cao
J. Mater. Sci. Technol. 186 (2024) 28-36
https://doi.org/10.1016/j.jmst.2023.10.046
134. Non-negligible role of gradient porous structure in superelasticity deterioration and improvement of NiTi shape memory alloys
JYintao Zhang, Daixiu Wei, Yang Chen, Lechun Xie, Liqiang Wang, Lai-Chang Zhang, Weijie Lu, Guang Chen
J. Mater. Sci. Technol. 186 (2024) 48-63
https://doi.org/10.1016/j.jmst.2023.10.053
135. Advanced high-entropy alloys breaking the property limits of current materials
Dongyue Li, Peter K. Liaw, Lu Xie, Yong Zhang, Wenrui Wang
J. Mater. Sci. Technol. 186 (2024) 219-230
https://doi.org/10.1016/j.jmst.2023.12.006
136. Fine grains with high-density annealing twins and precipitates inducing favorable strength and excellent plasticity in laser powder bed fusion-fabricated Inconel 718 via deep cryogenic and heat treatments
Bo Liu, Jiayu Xu, Yubi Gao, Yong Hu, Xiaokang Yang, Yutian Ding, Dong Zhang, Sujun Lu,
J. Mater. Sci. Technol. 187 (2024) 28-48
https://doi.org/10.1016/j.jmst.2023.11.030
137. Effect of austenitizing temperature on martensitic transformation in SA508Gr.4N steel
Shumeng Lu, Li Wan, Shanju Zheng, Mengnie Li, Juanna Ren, Baosheng Liu, Manal F. Abou Taleb, Zeinhom M. El-Bahy, Zhongdong Xu, Xiaojing Wang, Mohamed M. Ibrahim, Zhanhu Guo
J. Mater. Sci. Technol. 186 (2024) 244-255
https://doi.org/10.1016/j.jmst.2023.11.012
138. Room temperature growth of CsPbBr3 single crystal for asymmetric MSM structure photodetector
Longxing Su
J. Mater. Sci. Technol. 187 (2024) 113-122
https://doi.org/10.1016/j.jmst.2024.01.003
139. Fabrication of a novel Z-S-scheme photocatalytic fuel cell with the Z-scheme TiO2 /GO/g-C3N4 photoanode and S-scheme BiOAc1-xBrx/BiOBr photocathode for TC degradation
Tingting Yu, Bing Yang, Rong Zhang, Chenyu Yang, Arramel, Jizhou Jiang
J. Mater. Sci. Technol. 188 (2024) 11-26
https://doi.org/10.1016/j.jmst.2023.12.004
140. Morphological effects of WO3 in metal sulfide-based S-Scheme heterojunctions for boosting photocatalytic hydrogen production
Zhenkun Liu, Fei Jin, Xin Li, Peng Zhang, Zhiliang Jin
J. Mater. Sci. Technol. 188 (2024) 131-143
https://doi.org/10.1016/j.jmst.2023.10.060
141. In-situ generation of Au–carbon–TiO2 Ohmic junction from Ti3C2 MXene for efficient photocatalytic H2 evolution
Huanmin Liu, Chao Wu, Kangle Lv, Dingguo Tang, Qin Li
J. Mater. Sci. Technol. 188 (2024) 144-154
https://doi.org/10.1016/j.jmst.2023.12.012
142. Freestanding 1T MoS2 @MXene hybrid film with strong interfacial interaction for highly reversible zinc ions storage
Haonan Zhai, Huibin Liu, Yufen Zhang, Jinjin Wen, Wenyue Yang, Huiting Xu, Xiaoteng Yan, Wenchao Peng, Jiapeng Liu
J. Mater. Sci. Technol. 188 (2024) 183-190
https://doi.org/10.1016/j.jmst.2023.12.015
143. Eutectic high-entropy alloys and their applications in materials processing engineering: A review
Jinhong Liu, Zihan Li, Danyang Lin, Zhengxin Tang, Xiaoguo Song, Peng He, Shuye Zhang, Hong Bian, Wei Fu, Yanyu Song
J. Mater. Sci. Technol. 189 (2024) 211-246
https://doi.org/10.1016/j.jmst.2023.10.057
144. Multi-level hollow sphere rich in heterojunctions with dual function: Efficient microwave absorption and antiseptic
Liyuan Yu, Di Lan, Zhiqiang Guo, Ailing Feng, Guanglei Wu, Zirui Jia, Xing Feng, Pengfei Yin
J. Mater. Sci. Technol. 189 (2024) 155-165
https://doi.org/10.1016/j.jmst.2024.01.004
145. Fabrication of nitrogen-doped reduced graphene oxide/tricobalt tetraoxide composite aerogels with high efficiency, broadband microwave absorption, and good compression recovery performance
Ruiwen Shu, Lijuan Nie, Xinyue Liu, Ke Chen
J. Mater. Sci. Technol. 190 (2024) 106-116
https://doi.org/10.1016/j.jmst.2024.01.006
146. Ti3C2 -assisted construction of Z-scheme MIL-88A(Fe)/Ti3C2 /RF heterojunction: Multifunctional photocatalysis-in-situ-self-Fenton catalyst
Qi Wang, Hao Zhou, Jianying Qian, Biao Xue, Hao Du, Derek Hao, Yun Ji, Qiang Li
J. Mater. Sci. Technol. 190 (2024) 67-75
https://doi.org/10.1016/j.jmst.2023.11.045
147. Gradient nanostructure, enhanced surface integrity and fatigue resistance of Ti-6Al-7Nb alloy processed by surface mechanical attrition treatment
Hongwei Yang, Zichun Zhang, Jun Shu, Yong Han
J. Mater. Sci. Technol. 188 (2024) 252-269
https://doi.org/10.1016/j.jmst.2023.12.011
148. Recent progress in smart electromagnetic interference shielding materials
Xin Hou, Xue-Rong Feng, Ke Jiang, Yu-Chen Zheng, Jiang-Tao Liu, Ming Wang
J. Mater. Sci. Technol. 186 (2024) 256-271
https://doi.org/10.1016/j.jmst.2024.01.008
149. Robust liquid metal reinforced cellulose nanofiber/MXene composite film with Janus structure for electromagnetic interference shielding and electro-/photothermal conversion applications
Hui Zhao, Tong Gao, Jin Yun, Lixin Chen
J. Mater. Sci. Technol. 191 (2024) 23-32
https://doi.org/10.1016/j.jmst.2023.12.035
150. Bridging microstructure and crystallography with the crack propagation behavior in Ti-6Al-4V alloy fabricated via dual laser beam bilateral synchronous welding
Tingyan Yan, Yuan Liu, Jianfeng Wang, Yong Zheng, Xiaohong Zhan
J. Mater. Sci. Technol. 174 (2024) 1-14
https://doi.org/10.1016/j.jmst.2023.05.058
151. Mechanical tough and stretchable quaternized cellulose nanofibrils/MXene conductive hydrogel for flexible strain sensor with multi-scale monitoring
Qing-Yue Ni, Xiao-Feng He, Jia-Lin Zhou, Yu-Qin Yang, Zi-Fan Zeng, Peng-Fei Mao, Yu-Hang Luo, Jin-Meng Xu, Baiyu Jiang, Qiang Wu, Ben Wang, Yu-Qing Qin, Li-Xiu Gong, Long-Cheng Tang, Shi-Neng Li
J. Mater. Sci. Technol. 191 (2024) 181-191
https://doi.org/10.1016/j.jmst.2023.12.048
152. Thermophysical properties investigation of phase change microcapsules with low supercooling and high energy storage capability: Potential for efficient solar energy thermal management
Junfeng Shen, Yanqi Ma, Fan Zhou, Xinxin Sheng, Ying Chen
J. Mater. Sci. Technol. 191 (2024) 199-208
https://doi.org/10.1016/j.jmst.2024.01.014
153. Carbon dots-based nanocomposites for heterogeneous photocatalysis
Zhihan Yu, Fang Li, Quanjun Xiang
J. Mater. Sci. Technol. 175 (2024) 244-257
https://doi.org/10.1016/j.jmst.2023.08.023
154. Interface engineering and impedance matching strategy to develop core@shell urchin-like NiO/Ni@carbon nanotubes nanocomposites for microwave absorption
Tianming Jia, Yanling Hao, Xiaosi Qi, Yongchao Rao, Lei Wang, Junfei Ding, Yunpeng Qu, Wei Zhong
J. Mater. Sci. Technol. 176 (2024) 1-12
https://doi.org/10.1016/j.jmst.2023.08.022
155. Bioactivated polyetheretherketone scaffold able to generate mild heat for promoting bone regeneration via activating MAPK/ERK signaling pathway
Ce Zhu, Miaomiao He, Juehan Wang, Yong Huang, Wei Deng, Limin Liu, Ganjun Feng, Li Zhang, Yueming Song
J. Mater. Sci. Technol. 190 (2024) 188-199
https://doi.org/10.1016/j.jmst.2023.12.033
156. 2D/2D layered BiOIO3/g-C3N4 S-scheme heterojunction for photocatalytic NO oxidation
Xiaofeng Wu, Ningxin Kang, Xiaofang Li, Zhihua Xu, Sónia A.C. Carabineiro, Kangle Lv
J. Mater. Sci. Technol. 196 (2024) 40-49
https://doi.org/10.1016/j.jmst.2024.01.048
157. Constructing mixed-dimensional lightweight magnetic cobalt-based composites heterostructures: An effective strategy to achieve boosted microwave absorption and self-anticorrosion
Jiajun Li, Di Lan, Yuhang Cheng, Zirui Jia, Panbo Liu, Xuetao Shi, Hua Guo, Ailing Feng, Xing Feng, Guanglei Wu, Pengfei Yin
J. Mater. Sci. Technol. 196 (2024) 60-70
https://doi.org/10.1016/j.jmst.2024.02.016
158. Flowered molybdenum base trimetallic oxide decorated by CdS nanorod construct S-scheme heterojunctions for efficient photocatalytic hydrogen evolution
Jiayue Liu, Xueying Yang, Xin Guo, Zhiliang Jin
J. Mater. Sci. Technol. 196 (2024) 112-124
https://doi.org/10.1016/j.jmst.2024.01.058
159. Optimization of the in vitro biodegradability, cytocompatibility, and wear resistance of the AZ31B alloy by micro-arc oxidation coatings doped with zinc phosphate
Chao Yang, Suihan Cui, Ricky K.Y. Fu, Liyuan Sheng, Min Wen, Daokui Xu, Ying Zhao, Yufeng Zheng, Paul K. Chu, Zhongzhen Wu
J. Mater. Sci. Technol. 179 (2024) 224-239
https://doi.org/10.1016/jamst.2023.09.019
160. In situ X-ray imaging and numerical modeling of damage accumulation in C/SiC composites at temperatures up to 1200 °C
Weijian Qian, Wanen Zhang, Shengchuan Wu, Yue Hu, Xiangyu Zhang, Qiaodan Hu, Shaoming Dong, Shantung Tu
J. Mater. Sci. Technol. 197 (2024) 65-77
https://doi.org/10.1016/j.jmst.2024.01.069
161. 2D/2D Ti3C2 MXene/HTiNbO5 nanosheets Schottky heterojunction for boosting photothermal-assisted solar-driven photodegradation of tetracycline hydrochloride
Wen Xiao, Huan Yu, Chenghao Xu, Zhongyi Pu, Xiangyu Cheng, Fang Yu, Chao Liu, Qinfang Zhang, Zhigang Zou
J. Mater. Sci. Technol. 180 (2024) 193-206
https://doi.org/10.1016/j.jmst.2023.08.021
162. Elaborate construction of potent antioxidant properties in PBP-Ce( Ш ) nanosheets via a one-pot approach for seamless integration of anti-corrosion, wear-resistance, and flame-retardancy
Xiaoling He, Qihan Weng, Ruiqin Guo, Li Zhang, Xinxin Sheng, Delong Xie
J. Mater. Sci. Technol. 201 (2024) 197-209
https://doi.org/10.1016/j.jmst.2024.03.012
163. FeNi alloys incorporated N-doped carbon nanotubes as efficient bifunctional electrocatalyst with phase-dependent activity for oxygen and hydrogen evolution reactions
Yu Zhang, Boyuan Chen, Yanxin Qiao, Yurong Duan, Xinyu Qi, Siqi He, Hu Zhou, Junkang Chen, Aihua Yuan, Shunli Zheng
J. Mater. Sci. Technol. 201 (2024) 157-165
https://doi.org/10.1016/j.jmst.2024.03.046
164. Tailoring properties of directed energy deposited Al-Mg alloy by balancing laser shock peening and heat treatment
Wei Dai, Wei Guo, Jun Xiao, Ying Zhu, Zewu Qi, Jiaxin Shi, Changhao Yin, Dongsheng He, Jiaxuan Chi, Zhandong Wan, Baoqiang Cong, Minggao Li, Hongqiang Zhang
J. Mater. Sci. Technol. 203 (2024) 78-96
https://doi.org/10.1016/j.jmst.2024.03.051
165. Research progress of structural regulation and composition optimization to strengthen absorbing mechanism in emerging composites for efficient electromagnetic protection
Pengfei Yin, Di Lan, Changfang Lu, Zirui Jia, Ailing Feng, Panbo Liu, Xuetao Shi, Hua Guo, Guanglei Wu, Jian Wang
J. Mater. Sci. Technol. 204 (2024) 204-223
https://doi.org/10.1016/j.jmst.2024.04.007
166. Designing gadolinium-transition metals-based perovskite type high entropy oxides with good cryogenic magnetocaloric performances
Junli Lin, Xin Wang, Fengying Chen, Hai-Feng Li, Lingwei Li
J. Mater. Sci. Technol. 207 (2024) 317-323
https://doi.org/10.1016/j.jmst.2024.05.004
167. A bi-functional catalyst strategy to selectively regulate sulfur redox kinetics in lithium–sulfur batteries
Yanan Liu, Xiaoxiao Huang, Honglei Zhang, Guangyu Qin, Xiaoshuang Wang, Meixiu Song, Hongbo Liang, Jingzhe Hong, Yudong Huang
J. Mater. Sci. Technol. 180 (2024) 54-62
https://doi.org/10.1016/j.jmst.2023.07.024
2024年11月ESI热点论文
1. S/N-co-doped graphite nanosheets exfoliated via three-roll milling for high-performance sodium/potassium ion batteries
Xin Wang, Zhicong Luo, Juntong Huang, Zhi Chen, Tong Xiang, Zhijun Feng, Jing Wang, Sinong Wang, Yongcun Ma, Huiyong Yang, Xibao Li
J. Mater. Sci. Technol. 147 (2023) 47-55
https://doi.org/10.1016/j.jmst.2022.11.015
2. S-scheme heterojunction in photocatalytic hydrogen production
Teng Li, Noritatsu Tsubaki, Zhiliang Jin
J. Mater. Sci. Technol. 169 (2024) 82-104
https://doi.org/10.1016/j.jmst.2023.04.049
3. CuInS2 quantum-dot-modified g-C3N4 S-scheme heterojunction photocatalyst for hydrogen production and tetracycline degradation
Teng Li, Noritatsu Tsubaki, Zhiliang Jin
J. Mater. Sci. Technol. 172 (2024) 145-155
https://doi.org/10.1016/j.jmst.2023.06.042
4. Hollow engineering of sandwich NC@Co/NC@MnO2 composites toward strong wideband electromagnetic wave attenuation
Chenhao Wei, Lingzi Shi, Maoqing Li, Mukun He, Mengjie Li, Xinrui Jing, Panbo Liu, Junwei Gu
J. Mater. Sci. Technol. 175 (2024) 194-203
https://doi.org/10.1016/j.jmst.2023.08.020
5. A review of updated S-scheme heterojunction photocatalysts
Fangyi Li, Guihua Zhu, Jizhou Jiang, Lang Yang, Fengxia Deng, Arramel, Xin Li
J. Mater. Sci. Technol. 177 (2024) 142-180
https://doi.org/10.1016/j.jmst.2023.08.038
6. Multi-level hollow sphere rich in heterojunctions with dual function: Efficient microwave absorption and antiseptic
Liyuan Yu, Di Lan, Zhiqiang Guo, Ailing Feng, Guanglei Wu, Zirui Jia, Xing Feng, Pengfei Yin
J. Mater. Sci. Technol. 189 (2024) 155-165
https://doi.org/10.1016/j.jmst.2024.01.004
7. Ti3C2 -assisted construction of Z-scheme MIL-88A(Fe)/Ti3C2 /RF heterojunction: Multifunctional photocatalysis-in-situ-self-Fenton catalyst
Qi Wang, Hao Zhou, Jianying Qian, Biao Xue, Hao Du, Derek Hao, Yun Ji, Qiang Li
J. Mater. Sci. Technol. 190 (2024) 67-75
https://doi.org/10.1016/j.jmst.2023.11.045
8. Recent progress in smart electromagnetic interference shielding materials
Xin Hou, Xue-Rong Feng, Ke Jiang, Yu-Chen Zheng, Jiang-Tao Liu, Ming Wang
J. Mater. Sci. Technol. 186 (2024) 256-271
https://doi.org/10.1016/j.jmst.2024.01.008
9. In situ X-ray imaging and numerical modeling of damage accumulation in C/SiC composites at temperatures up to 1200 °C
Weijian Qian, Wanen Zhang, Shengchuan Wu, Yue Hu, Xiangyu Zhang, Qiaodan Hu, Shaoming Dong, Shantung Tu
J. Mater. Sci. Technol. 197 (2024) 65-77
https://doi.org/10.1016/j.jmst.2024.01.069
10. Elaborate construction of potent antioxidant properties in PBP-Ce( Ш ) nanosheets via a one-pot approach for seamless integration of anti-corrosion, wear-resistance, and flame-retardancy
Xiaoling He, Qihan Weng, Ruiqin Guo, Li Zhang, Xinxin Sheng, Delong Xie
J. Mater. Sci. Technol. 201 (2024) 197-209
https://doi.org/10.1016/j.jmst.2024.03.012
10. Advances in 2D/2D MXenes-based heterostructures for energy storage/conversion applications
Faiza Bibi, Irfan Ali Soomro, Abdul Hanan, Muhammad Nazim Lakhan, Amjad Khan, Naila Riaz Goraya, Zaeem Ur Rehman, Iftikhar Hussain, Kaili Zhang
J. Mater. Sci. Technol. 202 (2024) 82-118
https://doi.org/10.1016/j.jmst.2024.03.005
11. FeNi alloys incorporated N-doped carbon nanotubes as efficient bifunctional electrocatalyst with phase-dependent activity for oxygen and hydrogen evolution reactions
Yu Zhang, Boyuan Chen, Yanxin Qiao, Yurong Duan, Xinyu Qi, Siqi He, Hu Zhou, Junkang Chen, Aihua Yuan, Shunli Zheng
J. Mater. Sci. Technol. 201 (2024) 157-165
https://doi.org/10.1016/j.jmst.2024.03.046
12. Maneuverable B-site cation in perovskite tuning anode reaction kinetics in vanadium redox flow batteries
Yingqiao Jiang, Zihe Liu, Yujie Ren, Ao Tang, Lei Dai, Ling Wang, Suqin Liu, Yongguang Liu, Zhangxing He
J. Mater. Sci. Technol. 186 (2024) 199-206
https://doi.org/10.1016/j.jmst.2023.12.005
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。

官方微信
《腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62316606
- 邮箱:fsfhzy666@163.com
- 腐蚀与防护网官方QQ群:140808414