铝合金腐蚀的标准汇总(列表)
2025-08-12 14:56:32
作者:考拉腐蚀 来源:考拉腐蚀
分享至:
(1) ASTM G34-23 Standard test method for exfoliation corrosion(剥落腐蚀) susceptibility in 2XXX and 7XXX series Aluminum alloys(EXCO test)(2) ASTM G47-22 Standard Test Method for Determining Susceptibility to Stress Corrosion Cracking(应力腐蚀开裂) of 2XXX and 7XXX Aluminum Alloy Products(3) ASTM G66-23 Standard test method for visual assessment of exfoliation corrosion susceptibility of 5XXX series aluminum alloys(ASSET Test)(4) ASTM G67-18 Standard test method for determining the susceptibility to intergranular corrosion(晶间腐蚀) of 5XXX series aluminum alloys by mass loss after exxposure to Nitric Acid(NAMLT Test)(5) ASTM G69-20 Standard test method for measurement of corrosion potentials(腐蚀电位) of alluminum alloys(6) ASTM G103-1997R23(e1) Standard practice for evaluating stress corrosion cracking resistance of low copper 7XXX series Al-Zn-Mg-Cu alloys in boiling 6% sodium chloride solution (7) ASTM G110-92(2022)e2 Standrad practice for evaluating intergranular corrosion resistance of heat treable aluminum alloys by immersion in Sodium Chloride + Hydrogen Pereoxide solution(8) ASTM G112-2022 Standard Gudie for conducting exfoliation corrosion tests in aluminum alloys (9) ASTM G139-05(2022) Test Method for determining stress corrosion cracking resistance of heat-treable Aluminum Alloy products using Breaking Load method(10) GB/T 7998-2005 铝合金晶间腐蚀测定方法(Test method for intergranular corrosion of aluminum alloy),参考ASTM G110-1992
(11) GB/T 7998-2023 铝合金晶间腐蚀敏感性评价方法(Method for evaluating the suscetibility to intergranular corrosion of alumunum alloys),替代GB/T 79998-2005he GB/T 26491-2011《5XXXX系铝合金晶间腐蚀试验方法 质量损失法》,适用于2、5、6、7系铝合金产品晶间腐蚀敏感性的测定。(12) GB/T 22640-2023 铝合金应力腐蚀敏感性评价试验方法(Test method for determining susceptibility to stress corrosion cracking of aluminum alloys)适用于:C型环试样恒应变、弯梁试样恒应变、U型试样恒应变、拉伸试样恒载荷、拉伸试样恒应变、拉伸试样慢速率拉伸、沸腾氯化钠溶液恒应变等;(2系-Cu1.8%~7.0%、6系、7系-Cu0.4%~2.8%)(13) GB/T 26323-2010 色漆和清漆 铝及及合金表面涂膜的耐丝状腐蚀试验(Paints and varnishes - determination of resistance to filiform corrosion on aluminum and aluminum alloys( ISO 4623-2:2003 MOD)(14) GB/T 33883-2017 7XXX系铝合金应力腐蚀 沸腾氯化钠溶液法(铜含量低于1.2%)(15) GB/T 36174-2018 金属和合金的腐蚀 固溶热处理铝合金的耐晶间腐蚀性的测定( ISO 11846:1995,IDT)(16) GB/T 40388-2021 金属和合金的腐蚀 铝合金剥落腐蚀试验(ISO 11881:1999,MOD)(17) GB/T 41653-2022 金属和合金的腐蚀 热处理铝合金晶间腐蚀敏感性阳极试验方法( corrosion of metals and alloys - anodic test for evaluation of intergranular corrosion susceptibility of heat treatable aluminum alloys)ISO 15329:2006,MOD(18) GB/T 42514-2023 铝及铝合金阳极氧化膜及有机聚合物膜的腐蚀评定 图表法( ISO 8993:2018,NEQ)(19) GB/T 42544-2023 铝及铝合金阳极氧化膜及有机聚合物膜的腐蚀评定 栅格法(ISO 8994:2018,NEQ)(20) HB 5254-83 变形铝合金拉伸应力腐蚀试验方法(21) HB 5255-83 铝合金晶间腐蚀及晶间腐蚀倾向的测定(22) HB 5259-83 铝合金C环试样应力腐蚀试验方法(23) HB 5294-84 高强度铝合金双悬臂(DCB)试样应力腐蚀试验方法(24) MH/T 6071-2011 夹层腐蚀试验方法Test method for sandwich corrosion test(25) SH/T 0620-95 发动机冷却液对传热状态下的铸铝合金腐蚀测定法(等效采用ASTM D4340)(26) SJ 30046-2019 铝合金晶间腐蚀试验方法(27) SJ 30047-2019 铝合金剥落腐蚀试验方法(28) T/CCTAS 54-2023 轨道交通车辆用铝合金材料晶间腐蚀测定方法
(29) T/CCTAS 55-2023 轨道交通车辆用抗应力腐蚀铝合金材料过程控制要求
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。