| 1 | 加速腐蚀试验 accelerated corriosion test |
| 2 | 加速氧化 accelerated oxidation |
| 3 | 酸洗 acid cleaning |
| 4 | 酸洗清洁剂 acid picking |
| 5 | 酸洗清洁剂 acidic cleaner |
| 6 | 酸度 acidity |
| 7 | 活化 activity |
| 8 | 激化能 activation energy |
| 9 | 活化极化 activation polarization |
| 10 | 活化剂 activator |
| 11 | 活性的,活化的 active |
| 12 | 活化金属 active metals |
| 13 | 活化-钝化电池 active-passive cell |
| 14 | 活性区,活化区 active zone |
| 15 | 活度 activity |
| 16 | 优级海军黄铜 admiralty brass |
| 17 | 充气 aeration |
| 18 | 充气电池 aeration cell |
| 19 | 嗜氧菌 aerobic bacteria |
| 20 | 老化 aging |
| 21 | 老化作用 aging action |
| 22 | 大气污染 air pollution |
| 23 | 周浸试验 alternate immersion test |
| 24 | 厌氧菌 anaerobic bacteria |
| 25 | 厌氧菌腐蚀 anaerobic corrosion |
| 26 | 阴离子 anion |
| 27 | 阳极 anode |
| 28 | 阳极极化 anodic polarization |
| 29 | 阳极电流密度 anodic current density |
| 30 | 阳极氧化物膜 anodic oxide coating |
| 31 | 阳极保护 anodic protection |
| 32 | 阳极区电解质 anolyte |
| 33 | 耐侯性低合金钢 anti-weathering low alloy steel |
| 34 | 外加电位 applied potential |
| 35 | 水溶液腐蚀 aqueous corrosion |
| 36 | 人造海水 artificial seawater |
| 37 | 大气暴露试验 atmospheric exposure test |
| 38 | 大气腐蚀 atmospheric corrosion |
| 39 | 奥氏体不锈钢 austenitic stainless steel |
| 40 | 辅助电极 auxiliary electrode |
| 41 | 细菌腐蚀 bacteria corrosion |
| 42 | 贱金属 base metal |
| 43 | 双金属腐蚀 bimetallic corrosion |
| 44 | 甘汞电极 calomel electrode |
| 45 | 甘汞电极电位 calomel electrode potential |
| 46 | 碳化 carburizing |
| 47 | 阴极 cathode |
| 48 | 阴极保护 cathodic protection |
| 49 | 阴极极化 cathodic polarization |
| 50 | 阴极电流密度 cathodic current density |
| 51 | 阴极电流效率 cathodic current efficiency |
| 52 | 阴极区电解质 catholyte |
| 53 | 阳离子 cation |
| 54 | 碱脆 caustic embrittlement |
| 55 | 空泡作用 cavitation |
| 56 | 空泡腐蚀 cavitation corrosion |
| 57 | 空泡损伤 cavitation damage |
| 58 | 空泡磨蚀 cavitation erosion |
| 59 | 电池 cell |
| 60 | 渗镀,渗碳 cementation |
| 61 | 化学清洗 chemical cleaning |
| 62 | 化学转化涂层 chemical conversion coating |
| 63 | 化学钝化 chemical passivation |
| 64 | 化学镀 chemical(electroless)plating |
| 65 | 铬酸盐处理(铬化) chromating |
| 66 | 清洗液 cleaning solution |
| 67 | 浓差电池 concentration cell |
| 68 | 接触腐蚀 contact corrosion |
| 69 | 转换涂层 conversion coating |
| 70 | 恒变形 constant deflection |
| 71 | 恒载荷 constant load |
| 72 | 腐蚀 corrosion |
| 73 | 腐蚀-磨蚀 corrosion-erosion |
| 74 | 腐蚀疲劳 corrosion fatigue |
| 75 | 腐蚀电位 corrosion potential |
| 76 | 腐蚀控制 corrosion control |
| 77 | 腐蚀电流 corrosion current |
| 78 | 腐蚀电流密度 corrosion current density |
| 79 | 腐蚀疲劳开裂 corrosion fatigue cracking |
| 80 | 腐蚀疲劳极限 corrosion fatigue limit |
| 81 | 腐蚀产物 corrosion product |
| 82 | 腐蚀速率 corrosion rate |
| 83 | 腐蚀科学 corrosion science |
| 84 | 腐蚀试验 corrosion test |
| 85 | 腐蚀失重 corrosion weight loss |
| 86 | 腐蚀增重 corrosion weight gain |
| 87 | 电偶 couple |
| 88 | 电偶作用 couple action |
| 89 | 开裂 cracking |
| 90 | 龟裂 crazing |
| 91 | 缝隙腐蚀 crevice corrosion |
| 92 | 临界阳极电流密度 critical anodic current density |
| 93 | 临界浓度 critical concentration |
| 94 | 临界湿度 critical humidity |
| 95 | 晶体 crystal |
| 96 | 辅助电极 counter electrode |
| 97 | 电流密度 current density |
| 98 | 去活化作用 deactivation |
| 99 | 脱合金元素作用 dealloying |
| 100 | 脱铝 dealuminization |
| 101 | 去气 deaeration |
| 102 | 缺陷 defect |
| 103 | 脱脂 degreasing |
| 104 | 去矿化物质 demineralization |
| 105 | 去极化 depolarization |
| 106 | 腐蚀深度 depth of corrosion |
| 107 | 沉积物腐蚀 deposit corrosion |
| 108 | 脱锌 dezincification |
| 109 | 扩散 diffusion |
| 110 | 扩散电位 diffusion potential |
| 111 | 差异充气电池 differential aeration cell |
| 112 | 极限扩散电流密度diffusion limited current density |
| 113 | 电流 electric current |
| 114 | 电位 electric potential |
| 115 | 电化学电池 electrochemical cell |
| 116 | 电化学腐蚀 electrochemical corrosion |
| 117 | 电化学当量 electrochemical equivalent |
| 118 | 电极 electrode |
| 119 | 电极电位 electrode potential |
| 120 | 电极反应 electrode reaction |
| 121 | 电解质 electrolyte |
| 122 | 电解 electrolysis |
| 123 | 电解清洗 electrolytic cleaning |
| 124 | 电动序 electromotive force(Emf)series |
| 125 | 负电性电位 electropositive potential |
| 126 | 电泳沉积 electrophoretic deposition |
| 127 | 电镀 electroplating |
| 128 | 正电性电位 electropositive potential |
| 129 | 静电喷涂层 electrostatic coating |
| 130 | 脆化 embrittlement |
| 131 | 磨耗 erosion |
| 132 | 磨耗腐蚀(或冲击腐蚀) erosion-corrosion |
| 133 | 平衡电位 equilibrium potential |
| 134 | 腐蚀极化图 Evans diagram |
| 135 | 剥蚀 exfoliation corrosion |
| 136 | 交换电流密度 exchange current density |
| 137 | 暴露实验 exposure test |
| 138 | 疲劳 fatigue |
| 139 | 铁素体 ferrite |
| 140 | 铁素体不锈钢 ferrite stainless steel |
| 141 | 丝状腐蚀 filiform corrosion |
| 142 | 弗拉德电位 Flade potential |
| 143 | 剥层腐蚀 foliation |
| 144 | 膜 film |
| 145 | 微动腐蚀 fretting corrosion |
| 146 | 燃灰腐蚀 fuel ash corrosion |
| 147 | 电偶作用 galvanic action |
| 148 | 伽法尼电池 galvanic cell |
| 149 | 电偶腐蚀 galvanic corrosion |
| 150 | 电偶对 galvanic couple |
| 151 | 电偶序 galvanic series |
| 152 | 热镀锌 galvanizing |
| 153 | 恒电流的 galvanoststatic |
| 154 | 普遍(全面)腐蚀 general corrosion |
| 155 | 晶界裂纹 grain boundary crack |
| 156 | 晶粒 grain |
| 157 | 石墨化腐蚀 graphitic corrosion |
| 158 | 重量法 gravimetric methods |
| 159 | 绿锈 green rot |
| 160 | 哈氏合金 hastelloy |
| 161 | 热影响区 heat affected zone(HAZ) |
| 162 | 耐热钢 heat resistant steel |
| 163 | 热处理 heat treatment |
| 164 | 高温腐蚀 high temperature corrosion |
| 165 | 热腐蚀 hot corrosion |
| 166 | 热镀铝 hot-dip alumizing |
| 167 | 湿度 humidity |
| 168 | 氢腐蚀 hydrogen attack |
| 169 | 氢鼓泡 hydrogen blistering |
| 170 | 氢损伤 hydrogen damage |
| 171 | 氢电极 hydrogen electrode |
| 172 | 氢脆 hydrogen embrittlement |
| 173 | 氢致开裂 hydrogen induced cracking |
| 174 | 氢超电压 hydrogen overvoltage |
| 175 | 氢标 hydrogen scale |
| 176 | 浸泡实验 immersion test |
| 177 | 冲蚀 impingement corrosion |
| 178 | 因科乃尔 Inconel |
| 179 | 因科罗 Incoloy |
| 180 | 工业大气 industrial atmosphere |
| 181 | 缓蚀剂 inhibitor |
| 182 | 晶间裂纹 intergranular crack |
| 183 | 不溶性阳极 insoluble anode |
| 184 | 晶间腐蚀 intergranular corrosion |
| 185 | 延晶应力腐蚀断裂 intergranular stress corrosion cracking |
| 186 | 内氧化 interal oxidation |
| 187 | 内应力 interal stress |
| 188 | 例子浓差电池 ion concentration cell |
| 189 | 离子 ion |
| 190 | 离子注入 ion implantation |
| 191 | 刀线腐蚀 knife-line corrosion |
| 192 | 激光釉化 laser glazing |
| 193 | 层状腐蚀 layer corrosion |
| 194 | 晶格缺陷 lattic defect |
| 195 | 液态金属腐蚀 liquid metal corrosion |
| 196 | 局部作用 local action |
| 197 | 局部电池 local cell |
| 198 | 局部腐蚀 local corrosion |
| 199 | 海洋腐蚀 marine corrosion |
| 200 | 马氏体 martensite |
| 201 | 马氏体不锈钢 martensitic stainless steel |
| 202 | 力学性能 mechanical property |
| 203 | 金属离子浓差电池 metal ion concentration cell |
| 204 | 金属喷镀 metal spray |
| 205 | 金属镀层 metallic coating |
| 206 | 微生物腐蚀 microbiological corrosion |
| 207 | 金属粉化 metal dusting |
| 208 | 混合电位 mixed potential |
| 209 | 轧制铁鳞 mill scale |
| 210 | 贵金属 noble metal |
| 211 | 海军黄铜 navy brass |
| 212 | 贵电位 noble potential |
| 213 | 非金属涂层 nonmetallic coating |
| 214 | 氮化 nitriding |
| 215 | 过电位 overpotential |
| 216 | 氧化 oxidation |
| 217 | 开路电位 open circuit potential |
| 218 | 氧化-还原电位 oxidation-reduction potential |
| 219 | 氧化物 oxide |
| 220 | 氧化膜 oxide film |
| 221 | 氧浓差电池 oxygen concentration cell |
| 222 | 钝化 passivation |
| 223 | 钝化剂 passivator |
| 224 | 钝化-活化电池 passive-active cell |
| 225 | 钝化的,钝性的 passive |
| 226 | 铜绿 patina |
| 227 | 酸度计 pH indicator,acidometer |
| 228 | 磷酸盐处理 phosphating |
| 229 | 酸洗液 pickling solution |
| 230 | 蚀孔 pit |
| 231 | 点蚀 pitting |
| 232 | 点蚀击穿电位 pitting breakdown potential |
| 233 | 点蚀系数 pitting factor |
| 234 | 点蚀电位 pitting potential |
| 235 | 极化 polarization |
| 236 | 动电位 potential dynamic(potentiokinetic) |
| 237 | 恒电位仪 potentiostat |
| 238 | 恒电位 potentisostic |
| 239 | 电位-pH图 Pourbaix diagram,potential-pH diagram |
| 240 | 底涂层 prime coat |
| 241 | 保护电位 protective potential |
| 242 | 氧化-还原电位 redox potential |
| 243 | 还原 reduction |
| 244 | 参比电极 reference electrode |
| 245 | 相对湿度 relative humidity |
| 246 | 残余内应力 residua interal stress |
| 247 | 铁锈 rust |
| 248 | 防锈油 rust preventive oil |
| 249 | 牺牲阳极保护 sacrifice anode protection |
| 250 | 盐水喷雾试验 salt spray test |
| 251 | 喷砂 sand blasting |
| 252 | 饱和甘汞电极 saturated calomel electrode(SCE) |
| 253 | 氧化皮 scale |
| 254 | 季裂 season cracking |
| 255 | 选择性腐蚀 selective corrosion |
| 256 | 选择性氧化 selective oxidation |
| 257 | 自钝化 self passivation |
| 258 | 敏化热处理 sensitizing heat treatment |
| 259 | 喷丸 shot peening |
| 260 | 银-氯化银电极 silver-sliver chloride electrode |
| 261 | 慢应变速率 slow strain rate |
| 262 | 土壤腐蚀 soil corrosion |
| 263 | 剥离 spalling |
| 264 | 不锈钢 stainless steel |
| 265 | 标准电极电位 standard electrode potential |
| 266 | 标准氢电极 standard hydrogen electrode |
| 267 | 应变能 strain energy |
| 268 | 杂散电流腐蚀 stray current corrosion |
| 269 | 应力场强度因子 stress intensity factor |
| 270 | 应力腐蚀断裂 stress corrosion cracking(SCC) |
| 271 | 硫化 sulfidation |
| 272 | 表面氧化 surface oxidation |
| 273 | 表面处理 surface treatment |
| 274 | 皮下腐蚀 subsurface corrosion |
| 275 | 塔菲尔斜率 Tafel slope |
| 276 | 失泽 tarnish |
| 277 | 抗拉强度 tensile strength |
| 278 | 热偶腐蚀 thermogalvanic corrosion |
| 279 | 热力学 thermodynamics |
| 280 | 结瘤腐蚀 tuberculation |
| 281 | 穿晶腐蚀 transgranular corrosion |
| 282 | 穿晶应力腐蚀断裂 transgranular stress corrosion cracking |
| 283 | 过钝化 transpassive |
| 284 | 膜下腐蚀 underfilm corrosion |
| 285 | 均匀腐蚀 umiform corrosion |
| 286 | 水线腐蚀 waterline corrosion |
| 287 | 焊接腐蚀 weld decay |
| 288 | 湿度 humidity |
| 289 | 工作电极 working electrode |
更多关于材料方面、材料腐蚀控制、材料科普等方面的国内外最新动态,我们网站会不断更新。希望大家一直关注中国腐蚀与防护网http://www.ecorr.org
责任编辑:王元
《中国腐蚀与防护网电子期刊》征订启事
投稿联系:编辑部
电话:010-62313558-806
邮箱:fsfhzy666@163.com
中国腐蚀与防护网官方 QQ群:140808414
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
相关文章
无相关信息
官方微信
《腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62316606
- 邮箱:fsfhzy666@163.com
- 腐蚀与防护网官方QQ群:140808415